| https://www.eptac.com/faqs/ask-helena-leo/ask/soldering-iron-tip-temperature
. As for the alloy being used, the 63/37 is liquidus at 183C and the new RoHS alloys, such as SAC305 and Sn100C have a liquidus temperature around 215C
Lewis & Clark | http://www.lewis-clark.com/product-tag/delta-5-wave-solder/
: 2011 Operating System: Windows based Details: Dual pot-Lead and Lead Free Includes full pot of Lead Free –SN100C solder and Lead SN63/PB37 solder Carbon Steel Solder pots with high temperature protective coating Automatic solder addition for (2
Lewis & Clark | https://www.lewis-clark.com/product/vitronics-soltec-delta-5-6622cc-wave-soldering-system/
: 2011 Operating System: Windows based Details: Dual pot-Lead and Lead Free Includes full pot of Lead Free –SN100C solder and Lead SN63/PB37 solder Carbon Steel Solder pots with high temperature protective coating Automatic solder addition for (2
Lewis & Clark | http://www.lewis-clark.com/product/vitronics-soltec-delta-5-6622cc-wave-soldering-system/
: 2011 Operating System: Windows based Details: Dual pot-Lead and Lead Free Includes full pot of Lead Free –SN100C solder and Lead SN63/PB37 solder Carbon Steel Solder pots with high temperature protective coating Automatic solder addition for (2
Lewis & Clark | http://www.lewis-clark.com/product-category/wave-solder/
: 2011 Operating System: Windows based Details: Dual pot-Lead and Lead Free Includes full pot of Lead Free –SN100C solder and Lead SN63/PB37 solder Carbon Steel Solder pots with high temperature protective coating Automatic solder addition for (2
Lewis & Clark | http://www.lewis-clark.com/product-tag/vitronics-soltec/
: Windows based Details: Dual pot-Lead and Lead Free Includes full pot of Lead Free –SN100C solder and Lead SN63/PB37 solder Carbon Steel Solder pots with high temperature protective coating Automatic solder addition for (2
| https://www.eptac.com/faqs/ask-helena-leo/ask/solder-selection-for-printed-circuit-boards-and-terminals
. The alloys of SAC 305 and Sn100C will work together so mixing of those two should not be a problem. The concern, however; is the flux and can it be removed after the replacement of the component
| https://www.eptac.com/ask/solder-selection-for-printed-circuit-boards-and-terminals/
. The alloys of SAC 305 and Sn100C will work together so mixing of those two should not be a problem. The concern, however; is the flux and can it be removed after the replacement of the component
Lewis & Clark | http://www.lewis-clark.com/shop/page/27/
: 2011 Operating System: Windows based Details: Dual pot-Lead and Lead Free Includes full pot of Lead Free –SN100C solder and Lead SN63/PB37 solder Carbon Steel Solder pots with high temperature protective coating Automatic solder addition for (2