Technical Library | 2020-11-29 22:06:45.0
Plastic laminates are increasingly used as interposers within chip packaging applications. As a component within the package, the laminate is subjected to package moisture sensitivity testing. The moisture requirements of chip packaging laminates are related to ambient moisture absorption and thermal cycling. Printed wiring board (PWB) laminates, however, are gauged on properties relating to wet processes such as resist developing, copper etching, and pumice scrubbing. Consequently, printed wiring board moisture absorption test methods differ from chip packaging test conditions.
Technical Library | 2015-10-29 18:19:33.0
With the electronic industry moving towards lead-free assembly, traditional SnPb-compatible laminates need to be replaced with lead-free compatible laminates that can withstand the higher reflow temperature required by lead-free solders. Lead-free compatible laminates with improved heat resistance have been developed to meet this challenge but they are typically more brittle than SnPb laminates causing some to be more susceptible to pad cratering. In this paper, two novel approaches for minimizing pad cratering will be discussed. Preliminary results which validate the two approaches will also be presented.
Technical Library | 2022-04-28 06:42:19.0
I. Chip capacitors(MLCC) The full name of chip capacitors: multilayer (multilayer, laminated) chip ceramic capacitors, also known as chip capacitors, chip capacitance.
Technical Library | 2021-03-10 23:57:29.0
Latent short circuit failures have been observed during testing of Printed Circuit Boards (PCB) for power distribution of spacecraft of the European Space Agency. Root cause analysis indicates that foreign fibers may have contaminated the PCB laminate. These fibers can provide a pathway for electromigration if they bridge the clearance between nets of different potential in the presence of humidity attracted by the hygroscopic laminate resin. PCB manufacturers report poor yield caused by contamination embedded in laminate. Inspections show ...
Technical Library | 2013-05-16 15:52:00.0
In response to a growing concern within the Electronic Industry to the transition to Halogen-Free laminates (HFR-Free) within the Client Market space (Desktop and Notebook computers) iNEMI initiated a HFR-Free Leadership Workgroup to evaluate the readiness of the Industry to make this transition. The HFR-Free Leadership WG concluded that the electronic industry is ready for the transition and that the key electrical and thermo-mechanical properties of the new HFR-Free laminates can meet the required criteria. The HFR-Free Leadership WG verified that the laminate suppliers can meet the capacity demands for these new HFR-Free laminates and developed a "Test Suite Methodology" (TSM) that can facilitate the comparison and choice of the right laminate to replace brominated FR4 in the Client space... First published in the 2012 IPC APEX EXPO technical conference proceedings.
Technical Library | 2021-03-04 15:22:33.0
Copper clad laminates (CCLs) with low dissipation factor (Df) are urgently needed in the fields of high-frequency communications devices. A novel resin matrix of modified poly (2,6-dimethyl-1,4- phenylene ether) (MPPE) and styrene-ethylene/butylene-styrene (SEBS) was employed in the fabrication of high-frequency copper clad laminates (CCLs). The composites were reinforced by E-glass fabrics, which were modified with phenyltriethoxysilane (PhTES). The composite laminates obtained exhibited impressive dielectric loss of 0.0027 at 10 GHz when the weight ratio of MPPE to SEBS was 5:1.
Technical Library | 2012-07-19 21:24:02.0
First published in the 2012 IPC APEX EXPO technical conference proceedings. With the ever accelerating demands in printed circuit board (PCB) design, the choices of advanced laminate materials have become fewer and fewer. The trends continue towards high
Technical Library | 2009-04-30 18:06:24.0
This presentation surveys the most significant via and via-related laminate failure mechanisms from past to present using data from current induced thermal cycling (CITC) testing, failure analysis, and other sources. The relative life and failure modes of thru vias, buried vias, and microvias (stacked vs. non-stacked) are compared, along with the affect of structure, materials, and peak temperatures on the above. The origin of via-induced laminate failures such as "eyebrow cracks" and Pb free related internal delamination is also explored.
Technical Library | 2021-12-29 19:37:20.0
The purpose of this study was to compare the strength of the bond between resin and glass cloth for various composites (laminates) and its dependence on utilized soldering pad surface finishes. Moreover, the impact of surface finish application on the thermomechanical properties of the composites was evaluated. Three different laminates with various thermal endurances were included in the study. Soldering pads were covered with OSP and HASL surface finishes. The strength of the cohesion of the resin upper layer was examined utilizing a newly established method designed for pulling tests.
Technical Library | 2013-01-09 18:31:54.0
The increased temperatures associated with lead free processes have produced significant challenges for PWB laminates. Newly developed laminates have different curing processes, are commonly filled with ceramic particles or micro-clays and can have higher Tg values. These changes designed to reduce Z-axis expansion and improve the materials resistance to thermal excursions through primary attach and rework operations have also produced harder resin systems with reduced fracture toughness.