Effects Of Storage Environments On The Solderability Of Nickel Palladium- Gold Finish With Pb-Based And Pb- Free Solders

Technical Library | 2022-03-02 21:26:51.0

The solderability of a nickel-palladium-gold (Ni-Pd-Au) finish on a Cu substrate was evaluated for the Pb-free solder, 95.5Sn-3.9Ag-0.6 Cu (wt.%, abbreviated Sn-Ag-Cu) and the eutectic 63Sn-37 Pb (Sn-Pb) alloy. The solder temperature was 245ºC. The flux was a rosin-based mildly activated (RMA) solution. The Ni-Pd-Au finish was tested in the as-fabricated condition as well as after exposure to one of the following accelerated storage (shelf life) regiments: (1) 33.6, 67.2, or 336 hours in the Battelle Class 2 flowing gas environment or (2) 5, 16, or 24 hours of steam aging (88ºC, 90%RH).

Sandia National Laboratories

  1  

1.33 searches for Companies, Equipment, Machines, Suppliers & Information

Win Source Online Electronic parts

High Precision Fluid Dispensers
Void Free Reflow Soldering

Wave Soldering 101 Training Course
PCB Handling with CE

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
High Throughput Reflow Oven

World's Best Reflow Oven Customizable for Unique Applications
design with ease with Win Source obselete parts and supplies

Internet marketing services for manufacturing companies