Technical Library: 7..0 (Page 1 of 1)

Gold Embrittlement In Lead-Free Solder.

Technical Library | 2014-08-07 15:13:44.0

Gold embrittlement in SnPb solder is a well-known failure mechanism in electronic assembly. To avoid this issue, prior studies have indicated a maximum gold content of three weight percent. This study attempts to provide similar guidance for Pb-free (SAC305) solder. Standard surface mount devices were assembled with SnPb and SAC305 solder onto printed boards with various thicknesses of gold plating. The gold plating included electroless nickel immersion gold (ENIG) and electrolytic gold of 15, 25, 35, and 50 microinches over nickel. These gold thicknesses resulted in weight percentages between 0.4 to 7.0 weight percent.

DfR Solutions (acquired by ANSYS Inc)

  1  

7..0 searches for Companies, Equipment, Machines, Suppliers & Information

Best SMT Reflow Oven

World's Best Reflow Oven Customizable for Unique Applications
SMT feeders

High Precision Fluid Dispensers
Global manufacturing solutions provider

High Throughput Reflow Oven
Circuit Board, PCB Assembly & electronics manufacturing service provider

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.


"回流焊炉"