Pad Cratering Susceptibility Testing with Acoustic Emission

Technical Library | 2015-08-13 15:52:40.0

Pad cratering has become more prevalent with the switch to lead free solders and lead free compatible laminates. This mainly is due to the use of higher reflow temperature, stiffer Pb-free solder alloys, and the more brittle Pb-free compatible laminates. However, pad cratering is difficult to detect by monitoring electric resistance since pad cratering initiates before an electrical failure occurs. Several methods have been developed to evaluate laminate materials' resistance to pad cratering. Pad-solder level tests include ball shear, ball pull and pin pull. The detailed methods for ball shear, ball pull, and pin pull testing are documented in an industry standard IPC-9708. Bansal, et al. proposed to use acoustic emission (AE) sensors to detect pad cratering during four-point bend test. Currently there is an industry-working group working on test guidelines for acoustic emission measurement during mechanical testing.

Agilent Technologies, Inc.

  1  

agilent main searches for Companies, Equipment, Machines, Suppliers & Information

Solder Paste Dispensing

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.
Selective soldering solutions with Jade soldering machine

High Precision Fluid Dispensers
Hot selling SMT spare parts and professional SMT machine solutions

Training online, at your facility, or at one of our worldwide training centers"