Technical Library: amtech solder flux (Page 2 of 8)

Model for Improvement of Fluxing Process on Selective Soldering Machines

Technical Library | 2017-05-25 17:07:39.0

Purpose of this research is to identify the factors that directly influence the effectiveness of the fluxing process in selective soldering machines, using the design of experiment methodology with associated factors and levels used in the experiment. Final findings gives directions for set up of the optimal fluxing parameters that will enable appropriate flux appliance and to gain reduction of soldering quality issues which foundations are from this process.

Visteon Electronics

Can Age and Storage Conditions Affect the SIR Performance of a No-Clean Solder Paste Flux Residue?

Technical Library | 2017-02-09 17:08:44.0

The SMT assembly world, especially within the commercial electronics realm, is dominated by no-clean solder paste technology. A solder paste flux residue that does not require removal is very attractive in a competitive world where every penny of assembly cost counts. One important aspect of the reliability of assembled devices is the nature of the no-clean solder paste flux residue. Most people in this field understand the importance of having a process that renders the solder paste flux residue as benign and inert as possible, thereby ensuring electrical reliability.But, of all the factors that play into the electrical reliability of the solder paste flux residue, is there any impact made by the age of the solder paste and how it was stored? This paper uses J-STD-004B SIR (Surface Insulation Resistance) testing to examine this question.

Indium Corporation

Quieting the Noise: Quality Wave Soldering Depends on Control of Its Many Parameters.

Technical Library | 2008-01-24 16:19:43.0

The wave solder process is characterized by a large number of process parameters. To understand them all and their interactions is challenging, particularly when it comes to lead-free soldering. Wave soldering has a number of sub-processes, which include fluxing, preheating, soldering and cooling.

Vitronics Soltec

Laser Solder Reflow: A Process Solution Part I

Technical Library | 2007-09-06 11:03:33.0

EFD Inc. and Leister USA have collaborated to bust the myth that you cannot perform laser reflow with solder paste. Using Leister diode lasers, EFD has formulated solder pastes that survive the rapid reflow cycle typical of laser heating. These solder pastes reflow and wet well, without spatter, even when heating is accomplished in less than half a second. The flux core in wire solders cannot boast such flux spatter resistance in such an aggressive heating environment.

Nordson EFD

Understanding the Effect of Process Changes and Flux Chemistry on Mid-Chip Solder Balling

Technical Library | 2016-11-30 21:30:50.0

Mid-chip solder balling is a defect typically associated with solder paste exhibiting poor hot slump and/or insufficient wetting during the reflow soldering process, resulting in paste flowing under the component or onto the solder resist. Once molten, this solder is compressed and forced to the side of the component, causing mid-chip solder balling.This paper documents the experimental work performed to further understand the impact on mid-chip solder balling from both the manufacturing process and the flux chemistry.

Henkel Electronic Materials

Validity of the IPC R.O.S.E. Method 2.3.25 Researched

Technical Library | 2010-06-10 21:01:48.0

This paper researches the effectiveness of the R.O.S.E. cleanliness testing process for dissolving and measuring ionic contaminants from boards soldered with no-clean and lead-free flux technologies.

KYZEN Corporation

Simple, Effective Process Control in Wave Soldering

Technical Library | 1999-06-23 20:29:21.0

This paper outlines the harmful effects of out-of-control process parameters and describes methods of measuring and tracking them to keep them in control. It addresses all critical variables of wave soldering: flux deposition, preheat application, conveyor speed, solder temperature and solder contact time.

Siemens Process Industries and Drives

A Novel Epoxy Flux On Solder Paste For Assembling Thermally Warped POP

Technical Library | 2017-08-17 12:23:27.0

A novel epoxy flux EF-A was developed with good compatibility with no-clean solder pastes, and imparts high reliability for BGA assembly at a low cost. This compatibility with solder pastes is achieved by a well-engineered miscibility between epoxy and no-clean solder paste flux systems, and is further assured with the introduction of a venting channel. The compatibility enables a single bonding step for BGAs or CSPs, which exhibit high thermal warpage, to form a high-reliability assembly. Requirements in drop test, thermal cycling test (TCT), and SIR are all met by this epoxy flux, EF-A. The high viscosity stability at ambient temperature is another critical element in building a robust and userfriendly epoxy flux system. EF-A can be deposited with dipping, dispensing, and jetting. Its 75°C Tg facilitates good reworkability and minimizes the adverse impact of unfilled underfill material on TCT of BGA assemblies.

Indium Corporation

VOC-Free Wave Solder Flux Evaluation

Technical Library | 1999-04-26 15:51:30.0

The goal of the flux evaluation was to identify one product that would meet the needs of all SICN's wave solder products and processes while producing high quality assemblies. At the outset of the evaluation, it was unclear whether a single flux chemistry could satisfy such a broad range of demands, particularly because SICN's utilization of less aggressive, low-impact chemicals.

Siemens Process Industries and Drives

DOE for Process Validation Involving Numerous Assembly Materials and Test Methods.

Technical Library | 2010-03-18 14:02:03.0

Selecting products that have been qualified by industry standards for use in printed circuit board assembly processes is an accepted best practice. That products which have been qualified, when used in combinations not specifically qualified, may have resultant properties detrimental to assembly function though, is often not adequately understood. Printed circuit boards, solder masks, soldering materials (flux, paste, cored wire, rework flux, paste flux, etc.), adhesives, and inks, when qualified per industry standards, are qualified using very specific test methods which may not adequately mimic the assembly process ultimately used.

Trace Laboratories


amtech solder flux searches for Companies, Equipment, Machines, Suppliers & Information

Conductive Adhesive & Non-Conductive Adhesive Dispensing