Technical Library | 2016-05-26 15:07:36.0
The oxide layers are known as wetting inhibitors in component and PCB metallizations. The oxide acts as barrier that prevent the tin diffusion from happening. Besides, in corrosion studies, the role of salt residues -with Cl ion- on some metals is known as being promoters of oxidation or corrosion. On the other hand, most of corrosion studies with tin metallization are focused mainly on the corrosion resistance of tin alloys, but little has been done respecting to the influence of salts on tin metallization wetting. In this paper, a series of experiments was carried over to know the influence of specifically NaCl on BGA wetting given Head in Pillow (HiP) as result.
Technical Library | 2011-09-01 18:11:31.0
Scavenging, Site Dressing, Residual Solder Removal. What's in a name? "That which we call an onion, by any other name would smell as strong" (apologies to the immortal bard). And, regardless of the name you give it, the objective is the same, namely the clean up of remaining solder after a component (particularly a BGA) or R.F. Shield has been removed from a PCB. This paper will describe the various methods that are available and discuss their pros and cons.
Technical Library | 2015-03-04 10:56:26.0
As the proliferation of modern day electronics continues to drive miniaturization and functionality, electronic designers/assemblers face the issue of environmental exposure and uncommon applications never previously contemplated. This reality, coupled with the goal of reducing the environmental and health implications of the production and disposal of these devices, has forced manufacturers to reconsider the materials used in production. Furthermore, the need to increase package density and reduce costs has led to the rapid deployment of leadless packages such as QFN, POP, LGA, and Micro-BGA. In many cases, the manufacturers of these devices will recommend the use of no clean fluxes due to concerns over the ability to consistently remove flux residues from under and around these devices. These concerns, along with the need to implement a tin whisker mitigation strategy and/or increase environmental tolerance, have led to the conundrum of applying conformal coating over no clean residues.
1 |