Technical Library | 2023-07-22 02:26:05.0
Patch offset; Uneven patches throughout the substrate (each substrate is offset in a different way); Only part of the substrate is offset; Only certain components are offset; The patch Angle is offset; Component absorption error; Laser identification (component identification) error; Nozzle loading and unloading error; Mark (BOC mark, IC mark) identification error; Image recognition error (KE-2060 only); Analysis of the main reasons for throwing material. More information about KINGSUN please Contact US at jenny@ksunsmt.com or visit www.ksunsmt.com
Technical Library | 2018-04-27 13:23:31.0
When performing BGA component rework, it is important to know the actual heat that is coming out of the top and bottom heaters. This will be critical in setting up accurate heat profiles. Monitoring your heat output will also keep you aware of your heaters performance so that you will know when the heaters need to be replaced.
Technical Library | 2010-01-13 12:34:10.0
Micro-sectioning (sometimes referred to as cross-sectioning)is a technique, used to characterize materials or to perform a failure mode analysis, for exposing an internal section of a PCB or package. Destructive in nature, cross-sectioning requires encapsulation of the specimen in order to provide support, stability, and protection. Failures that can be investigated through micro-sectional analysis include component defects, thermo-mechanical failures, processing failures related to solder reflow, opens or shorts, voiding and raw material evaluations.
Technical Library | 2021-12-31 06:09:47.0
The packaging method of surface mount components has become an important part of the SMT system. It directly affects the efficiency of assembly production and must be optimized in combination with the type and number of feeders of the SMT machine. There are four main types of packaging for surface mount components, Tape, tube, tray and bulk.
Technical Library | 2023-11-20 17:42:33.0
Zero-defect strategies and increased demands on the production of assemblies are making quality assurance in electronics production increasingly important. Continous miniaturization of components, ever higher packing densities and the associated hard-to-view assembly areas, as well as the increased use of components such as BGAs, QFNs and QFPs, pose a considerable challenge when it comes to high-precision quality control.
Technical Library | 2024-06-19 14:23:36.0
These guidelines on long-term storage are intended to help develop a supply strategy for components which need to be warehoused, processed and used beyond ...
Technical Library | 2016-11-30 21:30:50.0
Mid-chip solder balling is a defect typically associated with solder paste exhibiting poor hot slump and/or insufficient wetting during the reflow soldering process, resulting in paste flowing under the component or onto the solder resist. Once molten, this solder is compressed and forced to the side of the component, causing mid-chip solder balling.This paper documents the experimental work performed to further understand the impact on mid-chip solder balling from both the manufacturing process and the flux chemistry.
Technical Library | 2003-04-18 12:05:57.0
The popular tin (Sn) rich lead free solders are causing severe corrosion to many of the materials used in today's Wave Solder systems. Users are experiencing higher maintenance frequency and reduced life of wave solder machine components. This paper describes the effects of Sn rich solders in contact with various materials and discusses alternate methods to alleviate this problem.
Technical Library | 2017-10-12 15:45:25.0
The risk associated with whisker growth from pure tin solderable terminations is fully mitigated when all of the pure tin is dissolved into tin-lead solder during SMT reflow. In order to take full advantage of this phenomenon, it is necessary to understand the conditions under which such coverage can be assured. A round robin study has been performed by IPC Task group 8-81f, during which identical sets of test vehicles were assembled at multiple locations, in accordance with IPC J-STD-001, Class 3. All of the test vehicles were analyzed to determine the extent of complete tin dissolution on a variety of component types. Results of this study are presented together with relevant conclusions and recommendations to guide high reliability end-users on the applicability and limitations of this mitigation strategy.
Technical Library | 2022-12-19 18:59:51.0
Material and Process Characterization studies can be used to quantify the harmful effects that might arise from solder flux and other process residues left on external surfaces after soldering. Residues present on an electronic assembly can cause unwanted electrochemical reactions leading to intermittent performance and total failure. Components with terminations that extend underneath the package can trap flux residue. These bottom terminated components are flush with the bottom of the device and can have small solderable terminations located along the perimeter sides of the package. The clearance between power and ground render high electrical forces, which can propagate electrochemical interactions when exposed to atmospheric moisture (harsh environments). The purpose of this research is to predict and understand the functional performance of residues present under single row QFN component packages. The objective of the research study is to develop and collect a set of guidelines for understanding the relationship between ionic contamination and electrical performance of a BTC component when exposed to atmospheric moisture and the trade-offs between electrical, ionic contamination levels, and cleanliness. Utilizing the knowledge gained from undertaking the testing of QFN components and associated DOE, the team will establish a reference Test Suite and Test Spec for cleanliness.
The SMTA membership is a network of professionals who build skills, share practical experience and develop solutions in electronic assembly technologies and related business operations.
Training Provider / Events Organizer / Association / Non-Profit
6600 City W Pkwy
Eden Prairie, MN USA
Phone: 952-920-7682