Whisker Formation Induced by Component and Assembly Ionic Contamination

Technical Library | 2023-02-13 18:56:42.0

This paper describes the results of an intensive whisker formation study on Pb-free assemblies with different levels of cleanliness. Thirteen types of as-received surface-mount and pin-through-hole components were cleaned and intentionally contaminated with solutions containing chloride, sulfate, bromide, and nitrate. Then the parts were assembled on double-sided boards that were also cleaned or intentionally contaminated with three fluxes having different halide contents. The assemblies were subjected to high-temperature/high-humidity testing (85_C/85% RH). Periodic examination found that contamination triggered whisker formation on both exposed tin and solder fillets. Whisker occurrence and parameters depending on the type and level of contamination are discussed. Cross-sections were used to assess the metallurgical aspects of whisker formation and the microstructural changes occurring during corrosion.

Celestica Corporation

DoD/EPA/DOE SERDP WP-2213: Novel Whisker Mitigating Composite Conformal Coat Assessment

Technical Library | 2023-02-13 19:14:03.0

Technology Focus: Develop and evaluate nanoparticle filled conformal coatings designed to provide long term whisker penetration resistance and coverage on tin rich metal surfaces prone to whisker growth in commercial lead-free electronics used in modern DoD systems. Research Objectives: Identify the fundamental mechanisms by which conformal coatings provide long-term tin whisker penetration resistance and inhibit nucleation/growth. Correlate mechanical properties and coverage thickness to whisker penetration resistance. Project Progress and Results: Functionalized nanosilica and non-functional nanoalumina enhanced polyurethane conformal coatings have shown improved spray coating coverage characteristics and crack resistance during thermal cycling fatigue testing. Lead-free assembly whisker mitigation validation testing is in process. Technology Transition: Current project partners provide coating materials to industry. SERDP test data will be considered during updates to the DoD adopted IPC standards for coating materials and coverage.

BAE SYSTEMS

An Investigation of Whisker Growth on Tin Coated Wire and Braid

Technical Library | 2012-08-02 21:05:14.0

First published in the 2012 IPC APEX EXPO technical conference proceedings. Pure tin is a common finish for copper hook up wire, coaxial cable, ground braid and harness assemblies used on electronic assemblies. Historically there have been fewer reports o

Rockwell Collins

Tin Whisker Risk Mitigation for High-Reliability Systems Integrators and Designers

Technical Library | 2015-06-04 19:10:47.0

Integrators and designers of high-reliability systems exert little or no control over component-level plating processes that affect the propensity for tin whiskering. Challenges of how to assure long-term reliability, while continuing to use COTS parts plated with pure tin, continue to arise. An integrated, quantitative, standardized methodology is proposed whereby mitigation levels can be selected that are appropriate for specific applications of pure tin for given end-uses. A system of hardware end-use classification is proposed, together with recommended appropriate risk mitigation approaches. An updated version of the application-specific risk assessment algorithm is presented together with recommended thresholds for acceptability within the context of the hardware classifications.

Raytheon

Sample Preparation For Mitigating Tin Whiskers In Alternative Lead-Free Alloys

Technical Library | 2016-02-18 18:55:09.0

As lead-free alloys shift into high reliability electronics, the issue of tin whisker growth remains a primary concern among those in the industry. Current research shows that there is no perfect alloy for all cases of electronic usage. Industry leaders and researchers continue to study and search for a lead free alloy that is able to withstand harsh environments while maintaining high reliability.

AIM Solder

Mitigation of Pure Tin Risk by Tin-Lead SMT Reflow- Results of an Industry Round-Robin

Technical Library | 2017-10-12 15:45:25.0

The risk associated with whisker growth from pure tin solderable terminations is fully mitigated when all of the pure tin is dissolved into tin-lead solder during SMT reflow. In order to take full advantage of this phenomenon, it is necessary to understand the conditions under which such coverage can be assured. A round robin study has been performed by IPC Task group 8-81f, during which identical sets of test vehicles were assembled at multiple locations, in accordance with IPC J-STD-001, Class 3. All of the test vehicles were analyzed to determine the extent of complete tin dissolution on a variety of component types. Results of this study are presented together with relevant conclusions and recommendations to guide high reliability end-users on the applicability and limitations of this mitigation strategy.

Raytheon

Solderability after Long-Term Storage

Technical Library | 2022-03-02 20:51:50.0

The effect of long-term storage on manufacturability and reliability is an area of major concern for companies that attempt to proactively manage component availability and obsolescence. A number of issues can arise depending on the technology and storage environment. Mechanisms of concern can include solderability, stress driven diffusive voiding, kirkendahl voiding, and tin whiskering. Of all of these, solderability / wettability remains the number one challenge in longterm storage.

DfR Solutions

Conformal Coating over No Clean Flux Residues

Technical Library | 2015-03-04 10:56:26.0

As the proliferation of modern day electronics continues to drive miniaturization and functionality, electronic designers/assemblers face the issue of environmental exposure and uncommon applications never previously contemplated. This reality, coupled with the goal of reducing the environmental and health implications of the production and disposal of these devices, has forced manufacturers to reconsider the materials used in production. Furthermore, the need to increase package density and reduce costs has led to the rapid deployment of leadless packages such as QFN, POP, LGA, and Micro-BGA. In many cases, the manufacturers of these devices will recommend the use of no clean fluxes due to concerns over the ability to consistently remove flux residues from under and around these devices. These concerns, along with the need to implement a tin whisker mitigation strategy and/or increase environmental tolerance, have led to the conundrum of applying conformal coating over no clean residues.

AIM Solder