Technical Library: lamination (Page 2 of 5)

Investigation of Impacts on Printed Circuit Board Laminated Composites Caused by Surface Finish Application

Technical Library | 2021-12-29 19:37:20.0

The purpose of this study was to compare the strength of the bond between resin and glass cloth for various composites (laminates) and its dependence on utilized soldering pad surface finishes. Moreover, the impact of surface finish application on the thermomechanical properties of the composites was evaluated. Three different laminates with various thermal endurances were included in the study. Soldering pads were covered with OSP and HASL surface finishes. The strength of the cohesion of the resin upper layer was examined utilizing a newly established method designed for pulling tests.

Czech Technical University in Prague

The Application of Spherical Bend Testing to Predict Safe Working Manufacturing Process Strains

Technical Library | 2013-01-09 18:31:54.0

The increased temperatures associated with lead free processes have produced significant challenges for PWB laminates. Newly developed laminates have different curing processes, are commonly filled with ceramic particles or micro-clays and can have higher Tg values. These changes designed to reduce Z-axis expansion and improve the materials resistance to thermal excursions through primary attach and rework operations have also produced harder resin systems with reduced fracture toughness.

Celestica Corporation

MECHANICAL FAILURES IN PB-FREE PROCESSING: EVALUATING THE EFFECT OF PAD CRATER DEFECTS ON PROCESS STRAIN LIMITS FOR BGA DEVICES

Technical Library | 2022-10-11 20:15:14.0

The increased temperatures associated with Pb-free processes have produced significant challenges for PWB laminates. Newly developed laminates have different curing processes, are commonly filled with ceramic particles or micro-clays and can have higher Tg values. These changes which are aimed at improving the materials resistance to thermal excursions and maintaining electrical integrity through primary attach and rework operations have also had the effect of producing harder resin systems with lower fracture toughness.

Celestica Corporation

Analysis of Laminate Material Properties for Correlation to Pad Cratering

Technical Library | 2016-10-20 18:13:34.0

Pad cratering failure has emerged due to the transition from traditional SnPb to SnAgCu alloys in soldering of printed circuit assemblies. Pb-free-compatible laminate materials in the printed circuit board tend to fracture under ball grid array pads when subjected to high strain mechanical loads. In this study, two Pb-free-compatible laminates were tested, plus one dicycure non-Pb-free-compatible as control. One set of these samples were as-received and another was subjected to five reflows. It is assumed that mechanical properties of different materials have an influence on the susceptibility of laminates to fracture. However, the pad cratering phenomenon occurs at the layer of resin between the exterior copper and the first glass in the weave. Bulk mechanical properties have not been a good indicator of pad crater susceptibility. In this study, mechanical characterization of hardness and Young’s modulus was carried out in the critical area where pad cratering occurs using nano-indentation at the surface and in a cross-section. The measurements show higher modulus and hardness in the Pb-free compatible laminates than in the dicy-cured laminate. Few changes are seen after reflow – which is known to have an effect -- indicating that these properties do not provide a complete prediction. Measurements of the copper pad showed significant material property changes after reflow.

CALCE Center for Advanced Life Cycle Engineering

Evaluation of Laminates in Pb-free HASL Process and Pb-free Assembly Environment

Technical Library | 2012-09-20 21:45:38.0

First published in the 2012 IPC APEX EXPO technical conference proceedings. An evaluation of four FR4 laminates in commonly used stack-ups was done to determine their survivability for the Pb-free HASL process followed by a worst case Pb-free manufacturin

Agilent Technologies, Inc.

An Experimental Investigation of Fracture Toughness and Volume Resistivity of Symmetric Laminated Epoxy/ Glass Fiber/CNT multiscale composites

Technical Library | 2022-01-26 15:26:56.0

In this work an attempt is made to improve the fracture toughness and electrical conductivity of epoxy/glass fiber based laminates by the inclusion of carbon nanotube (CNT) fillers. The fiber orientation of the epoxy/ glass fiber (GF) fabric laminates was optimized based on estimation of mechanical properties. The carboxylic acid functionalized CNTs were incorporated into epoxy matrix by ultra-sonication method. The nano filled epoxy resin was used to prepare laminates with 30/45 GF fabric orientation. The CNT content was varied and its effect on the tensile properties was determined. The fracture toughness of multiphase composites was estimated using single edge notch bend (SENB) test. The presence of CNTs improved the fracture toughness by a crack bridging mechanism. The volume resistivity of multiphase composites was found to be superior to the conventional epoxy/CNT composite. The presence of glass fabric reduces the number of inter-tube contacts contributing to the reduction in volume resistivity.

Amrita University

Reliability of Embedded Planar Capacitors under Temperature and Voltage Stress

Technical Library | 2015-05-21 18:46:31.0

In this work the reliability of an embedded planar capacitor laminate under temperature and voltage stress is investigated. The capacitor laminate consisted of an epoxy-BaTiO3 composite sandwiched between two layers of copper. The test vehicle with the embedded capacitors was subjected to a temperature of 125oC and a voltage bias of 200 V for 1000 hours. Capacitance, dissipation factor, and insulation resistance were monitored in-situ. Failed capacitors exhibited a sharp drop in insulation resistance, indicating avalanche breakdown. The decrease in the capacitance after 1000 hours was no more than 8% for any of the devices monitored. The decrease in the capacitance was attributed to delamination in the embedded capacitor laminate and an increase in the spacing between the copper layers.

CALCE Center for Advanced Life Cycle Engineering

Pad Cratering Susceptibility Testing with Acoustic Emission

Technical Library | 2015-08-13 15:52:40.0

Pad cratering has become more prevalent with the switch to lead free solders and lead free compatible laminates. This mainly is due to the use of higher reflow temperature, stiffer Pb-free solder alloys, and the more brittle Pb-free compatible laminates. However, pad cratering is difficult to detect by monitoring electric resistance since pad cratering initiates before an electrical failure occurs. Several methods have been developed to evaluate laminate materials' resistance to pad cratering. Pad-solder level tests include ball shear, ball pull and pin pull. The detailed methods for ball shear, ball pull, and pin pull testing are documented in an industry standard IPC-9708. Bansal, et al. proposed to use acoustic emission (AE) sensors to detect pad cratering during four-point bend test. Currently there is an industry-working group working on test guidelines for acoustic emission measurement during mechanical testing.

Agilent Technologies, Inc.

Practical Fiber Weave Effect Modeling

Technical Library | 2011-03-16 20:05:15.0

Fiber weave effect is becoming more of an issue as bit rates continue to sore upwards to 5GB/s and beyond. Due to the non-homogenous nature of printed circuit board laminates, the fiberglass weave pattern causes signals to propagate at different speeds wi

Lamsim Enterprises Inc.

A Novel Material for High Layer Count and High Reliability Printed Circuit Boards

Technical Library | 2012-09-27 19:50:01.0

First published in the 2012 IPC APEX EXPO technical conference proceedings. Over the past few years a new family of laminate systems has been developed to face the increasing physical demands of withstanding Pb-free soldering processes used in the assembl

Shengyi Technology Co., Ltd.


lamination searches for Companies, Equipment, Machines, Suppliers & Information