Technical Library | 2019-02-20 16:35:24.0
The High Density Packaging (HDP) User Group has completed a project evaluating the high frequency loss impacts of a variety of imaged core surface treatments (bond enhancement treatments, including chemical bonding and newer low etch alternative oxides) applied just prior to press lamination. Initial high frequency Dk/Df electrical test results did not show a strong correlation with any of the methods utilized within this project to measured surface roughness. The more significant factor affecting the measured loss is the choice of pre-lamination surface treatment. Most of the new chemical treatment systems outperform the older existing systems which depend upon surface roughness techniques to promote adhesion.
1 |