Characteristics of Metals Leached from Waste Printed Circuit Boards Using Acidithiobacillus ferrooxidans

Technical Library | 2021-06-07 19:10:16.0

The aim of this study was to compare leaching characteristics of metals from printed circuit boards (PCBs), taken from waste electrical and electronic equipment in the presence and in the absence of the iron-oxidizing bacteria, Acidithiobacillus ferrooxidans. A. ferrooxidans not only increases the leached concentration of Cu from the PCBs, but also inhibits the components of the 0K medium and leached Cu from forming precipitates such as libethenite (Cu2(PO4)(OH)), thereby assisting Cu recovery from the PCBs. In addition, the leached concentration of Pb from PCBs decreased in the presence of A. ferrooxidans, due to Pb forming amorphous precipitates. It is expected that Pb is not highly toxic to A. ferrooxidans. Consequently, A. ferrooxidans can be used as a cost-effective and environmentally friendly way to leach out valuable metals from PCBs as low-grade urban ore.

Semyung University

Multilayer Ceramic Capacitors: Mitigating Rising Failure Rates

Technical Library | 2018-12-05 14:52:23.0

The multilayer ceramic capacitor (MLCC) has become a widely used electronics component both for surface mount and embedded PCB applications. The MLCC technologies have gone through a number of material and process changes such as the shift from precious metal electrode (PME) configurations which were predominantly silver/palladium to base metal electrodes (BME) dominated by nickel. Each of these changes were accompanied by both quality and reliability problems. The MLCC industry is now in the midst of an unprecedented set of challenges similar to the Moore’s Law challenges being faced by the semiconductor industry. While capacitor failures have historically been responsible for a significant percentage of product field failures (most estimates are ~30%) we are seeing disturbing developments in the low voltage (

DfR Solutions (acquired by ANSYS Inc)

Effect of Gold Content on the Microstructural Evolution of SAC305 Solder Joints Under Isothermal Aging

Technical Library | 2013-08-29 19:52:43.0

Au over Ni on Cu is a widely used printed circuit board (PCB) surface finish, under bump metallization (UBM), and component lead metallization. It is generally accepted that less than 3 wt.% Au in Sn-Pb solder joints inhibits formation of detrimental intermetallic compounds (IMC). However, the critical limit for Au content in Pb-free solder joints is not well established. Three surface-mount package platforms, one with a matte Sn surface finish and the others with Ni/Au finish, were soldered to Ni/Au-finished PCB using Sn-3.0Ag 0.5Cu (SAC305) solder, in a realistic manufacturing setting. The assembled boards were divided into three groups: one without any thermal treatment, one subjected to isothermal aging at 125°C for 30 days, and the third group aged at 125°C for 56 days...

Agilent Technologies, Inc.

Printed Electronics: Manufacturing Technologies and Applications

Technical Library | 2023-03-13 19:35:47.0

Translational Research in Additive Manufacturing at GTMI * Additive manufacturing/3D printing process and equipment development (e.g., metal, polymer and composites part manufacturing) * Computational modeling and simulation of additive manufacturing/printed electronics processes * Advanced materials development for additive manufacturing/printed electronics * Application development and demonstration of additive manufacturing/printed electronics

Georgia Institute of Technology

Conformal Coating Defects

Technical Library | 2023-07-04 17:31:22.0

Conformal Coatings are polymeric materials used to protect circuitry, parts, and related components. They are most commonly used to protect printed circuit boards (PCBs) and electronic devices. However, conformal coatings can be applied to a wide variety of materials, including metal, plastic, silicone, ceramics, glass, and even paper. We use the term "substrate" to refer to an object or material that's been coated with a conformal coating.

Diamond MT

Soldering to Gold Over Nickel Surfaces

Technical Library | 1999-05-07 11:28:39.0

There are many things that can go wrong when soldering to gold plate over nickel surfaces. First of all, we know that gold and solder are not good friends, as any time solder comes into contact with gold, something seems to go wrong. Either the solder bonds to the gold and eventually pulls off as the tin and gold cross-migrate, leaving voids; or the solder completely removes the gold and is expected to bond to the metal which was under the gold.

Kester

Reduced Oxide Soldering Activation (ROSA)

Technical Library | 2007-07-19 15:15:11.0

ROSA is a surface restoration technique that removes hard to reduce species like metal oxides or sulfides. At the time of its development, the focus was on solderability and compliance to environmental regulations. Industry trends and regulatory changes as a result of the Montreal Protocol were the driver for much of the concern over environmental compliance. The result was an increase in the development of no-clean and water soluble fluxes and the removal of halogenated cleaning chemistries.

Electronics Manufacturing Productivity Facility (EMPF)

Liquid Tin Corrosion and Lead Free Wave Soldering

Technical Library | 2008-02-12 22:52:41.0

Corrosion of solder pots and solder pot components in wave soldering equipment has been reduced with the introduction of corrosion resistant coatings and improved lead free solder alloys. The latest trends in protecting wave solder machine components from liquid metal corrosion by lead free solder alloys will be presented in order to provide guidelines for evaluating existing equipment as well as for purchasing new systems.

Speedline Technologies, Inc.

Joule Heating Effects on the Current Carrying Capacity of an Organic Substrate for Flip-Chip Applications

Technical Library | 2009-07-22 18:33:41.0

This paper deals with the thermal effects of joule heating in a high interconnect density, thin core, buildup, organic flip chip substrate. The 440 μm thick substrate consists of a 135 μm thick core with via density of about 200 μm. The typical feature sizes in the substrate are 50 micron diameter vias is the core/buildup layers and 12 micron thick metal planes. An experimental test vehicle is powered with current and the temperature rise was measured. A numerical model was used to simulate the temperature rise in the TV.

i3 Electronics

Ceramic to Plastic Packaging

Technical Library | 2010-04-15 22:06:32.0

As electronic products increase in functionality and complexity, there is an emphasis on affordability, miniaturization, and energy efficiency. The telecommunications, automotive, and commercial electronic markets are the leading drivers for these trends. These markets see high volume manufacturing with millions of units priced to the fraction of the cent. The choice of the packaging material for the electrical components for these markets can have a substantial effect on the cost of the final product. Therefore plastic encapsulated components are almost universally used in non-military applications over the conventional ceramic or metal electronic packages.

Electronics Manufacturing Productivity Facility (EMPF)


metallization searches for Companies, Equipment, Machines, Suppliers & Information

Circuit Board, PCB Assembly & electronics manufacturing service provider

World's Best Reflow Oven Customizable for Unique Applications
High Throughput Reflow Oven

Reflow Soldering 101 Training Course
SMT feeders

Wave Soldering 101 Training Course
Online Equipment Auction Jabil Monterrey MX Aug 19, 2024

Software for SMT placement & AOI - Free Download.
Hot selling SMT spare parts and professional SMT machine solutions

Private label coffee for your company - your logo & message on each bag!