Technical Library: pop (Page 2 of 3)

Characterization of Solder Defects on Package on Packages with AXI Systems for Inspection Quality Improvement

Technical Library | 2016-05-30 22:24:00.0

As a part of series of studies on X-Ray inspection technology to quantify solder defects in BGA balls, we have conducted inspection of 3 level POP package by using a new AXI that capable of 3D-CT imaging. The new results are compared with the results of earlier AXI measurements. It is found that 3D measurements offer better defect inspection quality, lower false call and escapes.

Flex (Flextronics International)

Assembly Reliability of TSOP/DFN PoP Stack Package

Technical Library | 2018-12-12 22:20:22.0

Numerous 3D stack packaging technologies have been implemented by industry for use in microelectronics memory applications. This paper presents a reliability evaluation of a particular package-on-package (PoP) that offers a reduction in overall PCB board area requirements while allowing for increases in functionality. It utilizes standard, readily available device packaging methods in which high-density packaging is achieved by: (1) using standard "packaged" memory devices, (2) using standard 3-dimensional (3-D) interconnect assembly. The stacking approach provides a high level of functional integration in well-established and already functionally tested packages. The stack packages are built from TSOP packages with 48 leads, stacked either 2-high or 4-high, and integrated into a single dual-flat-no-lead (DFN) package.

Jet Propulsion Laboratory

A Novel Low Temperature Fast Flow And Fast Cure Reworkable Underfill

Technical Library | 2014-04-11 16:03:15.0

In order to meet the increasing demand of device miniaturization, high speed, more memory, more function, low cost, and more flexibility in device design and manufacturing chain, underfilling has increasingly become an essential process for the good reliability of electronic devices. Filled capillary underfill has been selected for use in package-level where there is large thermal stress caused by CTE mismatch issue, but the underfill is usually not reworkable. Unfilled capillary underfill has been used for board-level application such as BGA/CSP, POP, WL-CSP where there is need for mechanical shock resistance, the underfill is usually reworkable.

YINCAE Advanced Materials, LLC.

Miniaturization with Help of Reduced Component to Component Spacing

Technical Library | 2015-03-12 18:26:16.0

Miniaturization and the integration of a growing number of functions in portable electronic devices require an extremely high packaging density for the active and passive components. There are many ways to increase the packaging density and a few examples would be to stack them with Package on Package (PoP), fine pitch CSP's, 01005 and last but not least reduced component to component spacing for active and passive components (...)This paper will discuss different layouts, assembly and material selections to reduce component to component spacing down to 100-125um (4-5mil) from today’s mainstream of 150-200um (6-8mil) component to component spacing.

Flex (Flextronics International)

A Low Cost Manufacturing Solution - Low Temperature Super-Fast Cure and Flow Reworkable Underfill

Technical Library | 2016-01-12 11:09:47.0

In order to meet the increasing demand of device miniaturization, high speed, more memory, more function, low cost, and more flexibility in device design and manufacturing chain, underfilling has increasingly become an essential process for the good reliability of electronic devices. Filled capillary underfill has been selected for used in package-level where there is large thermal stress caused by CTE mismatch issue, but the underfill is usually not reworkable. Unfilled capillary underfill has been used for board-level application such as BGA/CSP, POP, WL-CSP where there is need for mechanical shock resistance, the underfill is usually reworkable.

YINCAE Advanced Materials, LLC.

Package-on-Package (PoP) for Advanced PCB Manufacturing Process

Technical Library | 2021-12-16 01:45:05.0

In the 1990's, both BGA (Ball Grid Array) and CSP (Chip Size Package) are entering their end in the front-end packaging materials and process technology. Both BGA and CSP like SMD (Surface Mount Device) from the I 980's and THD (Through-Hole mount Device) from the 1970's are reaching its own impasse in terms of maximizing its electrical, mechanical, and thermal performances, size, weight, and reliability.

Samsung Electro-Mechanics

Conformal Coating over No Clean Flux Residues

Technical Library | 2015-03-04 10:56:26.0

As the proliferation of modern day electronics continues to drive miniaturization and functionality, electronic designers/assemblers face the issue of environmental exposure and uncommon applications never previously contemplated. This reality, coupled with the goal of reducing the environmental and health implications of the production and disposal of these devices, has forced manufacturers to reconsider the materials used in production. Furthermore, the need to increase package density and reduce costs has led to the rapid deployment of leadless packages such as QFN, POP, LGA, and Micro-BGA. In many cases, the manufacturers of these devices will recommend the use of no clean fluxes due to concerns over the ability to consistently remove flux residues from under and around these devices. These concerns, along with the need to implement a tin whisker mitigation strategy and/or increase environmental tolerance, have led to the conundrum of applying conformal coating over no clean residues.

AIM Solder

BVA: Molded Cu Wire Contact Solution for Very High Density Package-on- Package (PoP) Applications

Technical Library | 2015-01-28 17:39:34.0

Stacking heterogeneous semiconductor die (memory and logic) within the same package outline can be considered for less complex applications but combining the memory and processor functions in a single package has compromised test efficiency and overall package assembly yield. Separation and packaging the semiconductor functions into sections, on the other hand, has proved to be more efficient and, even though two interposers are required, more economical. The separated logic and memory sections are configured with the same uniform outline for vertical stacking (package-on-package). The most common configuration places the logic section as the base with second tier memory section soldered to a mating contact pattern. This paper addresses the primary technological challenges for reducing contact pitch and package-on-package interface technology.

Invensas Corporation

A Novel Epoxy Flux On Solder Paste For Assembling Thermally Warped POP

Technical Library | 2017-08-17 12:23:27.0

A novel epoxy flux EF-A was developed with good compatibility with no-clean solder pastes, and imparts high reliability for BGA assembly at a low cost. This compatibility with solder pastes is achieved by a well-engineered miscibility between epoxy and no-clean solder paste flux systems, and is further assured with the introduction of a venting channel. The compatibility enables a single bonding step for BGAs or CSPs, which exhibit high thermal warpage, to form a high-reliability assembly. Requirements in drop test, thermal cycling test (TCT), and SIR are all met by this epoxy flux, EF-A. The high viscosity stability at ambient temperature is another critical element in building a robust and userfriendly epoxy flux system. EF-A can be deposited with dipping, dispensing, and jetting. Its 75°C Tg facilitates good reworkability and minimizes the adverse impact of unfilled underfill material on TCT of BGA assemblies.

Indium Corporation

Addressing the Challenge of Head-In-Pillow Defects in Electronics Assembly

Technical Library | 2013-12-27 10:39:21.0

The head-in-pillow defect has become a relatively common failure mode in the industry since the implementation of Pb-free technologies, generating much concern. A head-in-pillow defect is the incomplete wetting of the entire solder joint of a Ball-Grid Array (BGA), Chip-Scale Package (CSP), or even a Package-On-Package (PoP) and is characterized as a process anomaly, where the solder paste and BGA ball both reflow but do not coalesce. When looking at a cross-section, it actually looks like a head has pressed into a soft pillow. There are two main sources of head-in-pillow defects: poor wetting and PWB or package warpage. Poor wetting can result from a variety of sources, such as solder ball oxidation, an inappropriate thermal reflow profile or poor fluxing action. This paper addresses the three sources or contributing issues (supply, process & material) of the head-in-pillow defects. It will thoroughly review these three issues and how they relate to result in head-in pillow defects. In addition, a head-in-pillow elimination plan will be presented with real life examples will be to illustrate these head-in-pillow solutions.

Indium Corporation


pop searches for Companies, Equipment, Machines, Suppliers & Information

Equipment Auction Automotive Electronics Supplier - Closure of Tier-One SMT Dvision: (10) ASM & Universal SMT Lines & Feeders Equipment as-new-as 2019! Dek | Koh Young | Speedline | Vitronics | Viscom

Best Reflow Oven
Global manufacturing solutions provider

Component Placement 101 Training Course
Selective soldering solutions with Jade soldering machine