KE-2050/KE-2060 Causes and Countermeasures of Patch Failure

Technical Library | 2023-07-22 02:26:05.0

Patch offset; Uneven patches throughout the substrate (each substrate is offset in a different way); Only part of the substrate is offset; Only certain components are offset; The patch Angle is offset; Component absorption error; Laser identification (component identification) error; Nozzle loading and unloading error; Mark (BOC mark, IC mark) identification error; Image recognition error (KE-2060 only); Analysis of the main reasons for throwing material. More information about KINGSUN please Contact US at jenny@ksunsmt.com or visit www.ksunsmt.com

DONGGUAN KINGSUN AUTOMATION TECHNOLOGY CO.,LTD

Understanding the Heat Output of your BGA Rework Station

Technical Library | 2018-04-27 13:23:31.0

When performing BGA component rework, it is important to know the actual heat that is coming out of the top and bottom heaters. This will be critical in setting up accurate heat profiles. Monitoring your heat output will also keep you aware of your heaters performance so that you will know when the heaters need to be replaced.

Precision PCB Services, Inc

Micro-Sectioning of PCBs for Failure Analysis

Technical Library | 2010-01-13 12:34:10.0

Micro-sectioning (sometimes referred to as cross-sectioning)is a technique, used to characterize materials or to perform a failure mode analysis, for exposing an internal section of a PCB or package. Destructive in nature, cross-sectioning requires encapsulation of the specimen in order to provide support, stability, and protection. Failures that can be investigated through micro-sectional analysis include component defects, thermo-mechanical failures, processing failures related to solder reflow, opens or shorts, voiding and raw material evaluations.

BEST Inc.

What are the packaging forms of electronic components

Technical Library | 2021-12-31 06:09:47.0

The packaging method of surface mount components has become an important part of the SMT system. It directly affects the efficiency of assembly production and must be optimized in combination with the type and number of feeders of the SMT machine. There are four main types of packaging for surface mount components, Tape, tube, tray and bulk.

Shenzhen Sewate Technology Co.,Ltd

What is the application of moisture proof dry cabinet?

Technical Library | 2019-04-11 05:59:57.0

Are your MSD safely stored? As humidity is found to be one of the key reasons for rejected products, many manufacturers are taking measures to control the humidity to increase their production efficiency and save the cost. In the industries of semi-conductor and electronics, the key section in which the rejected products are most probably to be made is that during the heating process of SMT, the IC(e.g.,PBGA,BGA,or TQFD) is likely to crack and thus cause non-effective welding because of the humidity. Climatest Symor® auto dry cabinet is the best solution to avoid the cracking and non#2;effective welding by dehumidifying the surface of your components. The dry unit can be used for 20 years without replacement,and controller is calibration free within 5 years.We attach dry cabinet application with different humidity range,welcome to download.

Symor Instrument Equipment Co.,Ltd

What is usage of Electronic dry cabinet?

Technical Library | 2019-08-19 23:55:20.0

Electronic dry cabinet for MSD storage Humidity is one of the key reasons for rejected products, many manufacturers are taking measures to control the humidity to increase production efficiency and save cost. In semiconductor and electronic industry, the key section of rejected products mostly happen during SMT heating process, Climatest Symor® auto dry cabinet is a superior solution to avoid the cracking. Warranty: two years with lifetime technical support

Symor Instrument Equipment Co.,Ltd

The Effects of Long-Term Storage on Solderability of Semiconductor Components

Technical Library | 2022-03-02 21:52:34.0

In today's consumer-driven electronic marketplace many products have a limited useful life and component suppliers are moving to shorter product lifecycles. However, there are several industries that require semiconductor components to have a much longer lifecycle. In many cases application lifecycles within the Industrial, Automotive, Medical, Aerospace and Defense sectors may extend up to 30 years or more. As a result, an ongoing component supply becomes critical to sustaining these applications throughout their useful lifecycle. For this reason, it is often a requirement that semiconductor components be stored for extended periods of time after production ends.

Rochester Electronics LLC

Basics of Industrial Control System and the Use of PLC

Technical Library | 2021-11-26 01:18:30.0

The components of industrial control system (ICS) can be roughly divided into two categories according to their location: control center equipment and remote site equipment.

OKmarts Industrial Parts Mall

Principles of Analog In-Circuit Testing

Technical Library | 2012-12-26 14:18:24.0

Passive components including resistors, capacitors, inductors, and circuit-protection devices compose the highest percentage of all devices that are populated on today’s PCB assemblies. However, the successful isolation and testing of these components during ICT is perhaps the most challenging and the least understood of all modern-day validation practices.

Teradyne

Miniaturization with Help of Reduced Component to Component Spacing

Technical Library | 2015-03-12 18:26:16.0

Miniaturization and the integration of a growing number of functions in portable electronic devices require an extremely high packaging density for the active and passive components. There are many ways to increase the packaging density and a few examples would be to stack them with Package on Package (PoP), fine pitch CSP's, 01005 and last but not least reduced component to component spacing for active and passive components (...)This paper will discuss different layouts, assembly and material selections to reduce component to component spacing down to 100-125um (4-5mil) from today’s mainstream of 150-200um (6-8mil) component to component spacing.

Flex (Flextronics International)

  1 2 3 4 5 6 7 8 9 10 Next

rejection of components searches for Companies, Equipment, Machines, Suppliers & Information

Solder Paste Dispensing

We offer SMT Nozzles, feeders and spare parts globally. Find out more
SMT feeders

High Precision Fluid Dispensers
2024 Eptac IPC Certification Training Schedule

High Throughput Reflow Oven