A Novel Solution for No-Clean Flux not Fully Dried under Component Terminations

Technical Library | 2017-08-17 12:28:30.0

At SMT assembly, flux outgassing/drying is difficult for devices with poor venting channel, and resulted in insufficiently dried/burnt-off flux residue for no-clean process. Examples including: Large low stand-off components such as QFN, LGA Components covered under electromagnetic shield which has either no or few venting holes Components assembled within cavity of board Any other devices with small open space around solder joints

Indium Corporation

Lead-free Rework Process For Chip Scale Packages

Technical Library | 2007-03-28 10:18:33.0

Legislation against the use of lead in electronics has been the driving force behind the use of lead-free solders, surface finishes, and component lead finishes. The major concern in using lead-free solders in the assembly and rework Chip Scale Packages (CSPs) is the relatively high temperatures that the components and the boards experience. Fine-pitch CSPs have very low standoff heights following assembly making inspection and rework of these components more difficult. One other concern pertinent to rework is the temperature of the neighboring components during rework. These issues, coupled with the limitations of rework equipment to handle lead-free reflow temperatures, make the task of reworking lead-free assemblies more challenging.

Universal Instruments Corporation

Common Process Defect Identification of QFN Packages

Technical Library | 2019-07-23 22:33:47.0

The Quad Flat Pack No Leads (QFN) style of leadless packaging [also known as a Land Grid Array (LGA)] is rapidly increasing in us e for wireless, automotive, telecom and many other areas becaus e of its low cost, low stand-off height and excellent thermal and electri cal properties. With the implementation of any new package type, there is always a learning curve for its use in design and processing as well as for the Process and Quality Engineers who have to get to grips with the challenges that these packages bring. Therefore, this paper will provide examples of the common process defects that can be seen with QFNs /LGAs when using optical and x-ray inspection as part of manufacturing quality control. Results of trials conducted on four PCB finishes and using vapour phase and convection reflow will be discussed.

Nordson DAGE

The Risk And Solution For No-Clean Flux Not Fully Dried Under Component Terminations the Risk And Solution For No-Clean Flux Not Fully Dried Under Component Terminations

Technical Library | 2020-11-24 23:01:04.0

The miniaturization trend is driving industry to adopting low standoff components or components in cavity. The cost reduction pressure is pushing telecommunication industry to combine assembly of components and electromagnetic shield in one single reflow process. As a result, the flux outgassing/drying is getting very difficult for devices due to poor venting channel. This resulted in insufficiently dried/burnt-off flux residue. For a properly formulated flux, the remaining flux activity posed no issue in a dried flux residue for no-clean process. However, when venting channel is blocked, not only solvents remain, but also activators could not be burnt off. The presence of solvents allows mobility of active ingredients and the associated corrosion, thus poses a major threat to the reliability. In this work, a new halogen-free no-clean SnAgCu solder paste, 33-76-1, has been developed. This solder paste exhibited SIR value above the IPC spec 100 MΩ without any dendrite formation, even with a wet flux residue on the comb pattern. The wet flux residue was caused by covering the comb pattern with 10 mm × 10 mm glass slide during reflow and SIR testing in order to mimic the poorly vented low standoff components. The paste 33-76-1 also showed very good SMT assembly performance, including voiding of QFN and HIP resistance. The wetting ability of paste 33-76-1 was very good under nitrogen. For air reflow, 33-76-1 still matched paste C which is widely accepted by industry for air reflow process. The above good performance on both non-corrosivity with wet flux residue and robust SMT process can only be accomplished through a breakthrough in flux technology.

Indium Corporation

New Approaches to Develop a Scalable 3D IC Assembly Method

Technical Library | 2016-08-11 15:49:59.0

The challenge for 3D IC assembly is how to manage warpage and thin wafer handling in order to achieve a high assembly yield and to ensure that the final structure can pass the specified reliability requirements. Our test vehicles have micro-bumped die having pitches ranging from 60um down to 30um. The high density of pads and the large die size, make it extremely challenging to ensure that all of the micro-bump interconnects are attached to a thin Si-interposer. In addition, the low standoff between the die and interposer make it difficult to underfill. A likely approach is to first attach the die to the interposer and then the die/interposer sub-assembly to the substrate. In this scenario, the die/interposer sub-assembly is comparable to a monolithic silicon die that can be flip chip attached to the substrate. In this paper, we will discuss various assembly options and the challenges posed by each. In this investigation, we will propose the best method to do 2.5D assembly in an OSAT(Outsourced Assembly and Test) facility.

Invensas Corporation

Partially-Activated Flux Residue Impacts on Electronic Assembly Reliabilities

Technical Library | 2016-12-29 15:37:51.0

The reliabilities of the flux residue of electronic assemblies and semiconductor packages are attracting more and more attention with the adoption of no-clean fluxes by majority of the industry. In recent years, the concern of "partially activated" flux residue and their influence on reliability have been significantly raised due to the miniaturization along with high density design trend, selective soldering process adoption, and the expanded use of pallets in wave soldering process. When flux residue becomes trapped under low stand-off devices, pallets or unsoldered areas (e.g. selective process), it may contain unevaporated solvent, "live" activators and metal complex intermediates with different chemical composition and concentration levels depending on the thermal profiles. These partially-activated residues can directly impact the corrosion, surface insulation and electrochemical migration of the final assembly. In this study, a few application tests were developed internally to understand this issue. Two traditional liquid flux and two newly developed fluxes were selected to build up the basic models. The preliminary results also provide a scientific approach to design highly reliable products with the goal to minimize the reliability risk for the complex PCB designs and assembly processes. This paper was originally published by SMTA in the Proceedings of SMTA International

Kester

Cleaning Flux Residue under Leadless Components using Objective Evidence to Determine Cleaning Performance

Technical Library | 2019-08-14 22:20:55.0

Cleanliness is a product of design, including component density, standoff height and the cleaning equipment’s ability to deliver the cleaning agent to the source of residue. The presence of manufacturing process soil, such as flux residue, incompletely activated flux, incompletely cured solder masks, debris from handling and processing fixtures, and incomplete removal of cleaning fluids can hinder the functional lifetime of the product. Contaminates trapped under a component are more problematic to failure. Advanced test methods are needed to obtain "objective evidence" for removing flux residues under leadless components.Cleaning process performance is a function of cleaning capacity and defined cleanliness. Cleaning performance can be influenced by the PCB design, cleaning material, cleaning machine, reflow conditions and a wide range of process parameters.This research project is designed to study visual flux residues trapped under the bottom termination of leadless components. This paper will research a non-destructive visual method that can be used to study the cleanability of solder pastes, cleaning material effectiveness for the soil, cleaning machine effectiveness and process parameters needed to render a clean part.

KYZEN Corporation

  1  

standoff searches for Companies, Equipment, Machines, Suppliers & Information

2024 Eptac IPC Certification Training Schedule

High Precision Fluid Dispensers
2024 Eptac IPC Certification Training Schedule

High Throughput Reflow Oven
SMT Machines

World's Best Reflow Oven Customizable for Unique Applications
PCB separator

Internet marketing services for manufacturing companies