Comparing Soldering Results of ENIG and EPIG Post Steam Exposure

Technical Library | 2020-11-15 21:01:24.0

ENIG, electroless nickel immersion gold is now a well-regarded finish used to enhance and preserve the solder-ability of copper circuits. EPIG, electroless palladium immersion gold, is a new surface finish also for enhancing and preserving solder-ability but with the advantage of eliminating Electroless Nickel from the deposit layer. This feature has become increasingly important with the increasing use of high frequeny PWB designs whereby nickel's magnetic properties are detrimental. We examine these two finishes and their respective soldering characteristics as plated and after steam aging and offer an explanation for the performance deviation.

Uyemura International Corporation

Effects Of Storage Environments On The Solderability Of Nickel Palladium- Gold Finish With Pb-Based And Pb- Free Solders

Technical Library | 2022-03-02 21:26:51.0

The solderability of a nickel-palladium-gold (Ni-Pd-Au) finish on a Cu substrate was evaluated for the Pb-free solder, 95.5Sn-3.9Ag-0.6 Cu (wt.%, abbreviated Sn-Ag-Cu) and the eutectic 63Sn-37 Pb (Sn-Pb) alloy. The solder temperature was 245ºC. The flux was a rosin-based mildly activated (RMA) solution. The Ni-Pd-Au finish was tested in the as-fabricated condition as well as after exposure to one of the following accelerated storage (shelf life) regiments: (1) 33.6, 67.2, or 336 hours in the Battelle Class 2 flowing gas environment or (2) 5, 16, or 24 hours of steam aging (88ºC, 90%RH).

Sandia National Laboratories