Head-in-Pillow BGA Defects

Head-in-Pillow BGA Defects Head-in-Pillow BGA Defects. Head-in-pillow (HiP), also known as ball-and-socket, is a solder joint defect where the solder paste deposit wets the pad, but does not fully wet the ball. This results in a solder joint

SMTnet Express July 11 - 2013, Subscribers: 26149

SMTnet Express July 11, 2013, Subscribers: 26149, Members: Companies: 13418, Users: 34911 Effect of BGA Reballing and its Influence on Ball Shear Strength by S. Manian Ramkumar Ph.D., Andrew J. Daya, Daniel B. Lewanda; Rochester Institute

Surface Insulation Resistance Testing. Results of Independent Testing for Best Inc. BGA Stencil Repair Rework Samples Solder Paste Reattachment

Surface Insulation Resistance Testing. Results of Independent Testing for Best Inc. BGA Stencil Repair Rework Samples Solder Paste Reattachment If you don't see the images, please visit online version at #Application

Strength of Lead-free BGA Spheres in High Speed Loading

Strength of Lead-free BGA Spheres in High Speed Loading Strength of Lead-free BGA Spheres in High Speed Loading Concern about the failure of lead-free BGA packages when portable devices such as cell phones are accidentally dropped and a general

SMT Express, Issue No. 3 - from SMTnet.com

SMT Express, Issue No. 3 - from SMTnet.com Volume 1, Issue No. 3 Wednesday, August 18, 1999 Featured Article Return to Front Page BGA REWORK Earl Moon Proof Of Design (POD) INTRODUCTION This article is written to ensure everyone interested


bga voids searches for Companies, Equipment, Machines, Suppliers & Information