SMTnet Express, September 7, 2017, Subscribers: 30,782, Members: Companies: 10,712, Users: 23,761 Challenges on ENEPIG Finished PCBs: Gold Ball Bonding and Pad Metal Lift Young K. Song and Vanja Bukva; Teledyne DALSA As a surface finish for PCBs
SMTnet Express, December 30, 2021, Subscribers: 26,039, Companies: 11,482, Users: 26,994 " ---> Effects of PCB Substrate Surface Finish and Flux on Solderability of Lead-Free SAC305 Alloy The solderability of the SAC305 alloy
Influence of Pd Thickness on Micro Void Formation of Solder Joints in ENEPIG Surface Finish SMTnet Express December 13, 2012, Subscribers: 26067, Members: Companies: 9068, Users: 34058 Influence of Pd Thickness on Micro Void Formation of Solder
Wire Bonding and Soldering on Enepig and Enep Surface Finishes with Pure Pd-Layers SMTnet Express October 11, 2012, Subscribers: 25550, Members: Companies: 9005, Users: 33789 Wire Bonding and Soldering on Enepig and Enep Surface Finishes with Pure