Electronics Forum | Wed Aug 27 17:12:34 EDT 2008 | mikesewell
Silicone contamination could appear as fisheyes or dark spots under UV light. 1A33 can be heat cured but is a single component oxygen cure coating - it needs a source of oxygen to cure. An unvented oven may slow or limit the cure. Check out the TDS
Electronics Forum | Fri Aug 07 16:45:35 EDT 2020 | duso02
All URs require a long time to fully cure. And actually, most users do not reach full-cure before using the board. Even Humiseal 1A33 will be dry enough to handle after a very short time.
Industry News | 2010-06-11 15:24:29.0
DENVER, CO — Krayden, Inc., a leading distributor of engineered materials, announces that the popular Humiseal UV40 conformal coating is now available as a gel.