Electronics Forum | Thu Sep 07 10:39:34 EDT 2006 | vicknesh28
Can u elaborate on the bad plating? Have u had any experience on this before? The component has 90/10 Tin lead plating
Electronics Forum | Fri Nov 07 15:57:56 EST 2003 | Marc Simmel
Are there specifications or recommendations for electro-deposited tin-lead plating thickness on austenitic stainless steel that would provide a shelf life of 1 year? 6 months? Would 2 to 3 microns (78 to 118 micro-inches) 90/10 tin-lead over 1.27 mi
Impact of Reflowing A Pb-free Solder Alloy Using A Tin/Lead Solder Alloy Reflow Profile On Solder Joint Integrity If you don't see images, please visit online version at #Application.SmtNet.baseURL#/express/ The Impact of Reflowing A Pb
GPD Global | https://www.gpd-global.com/component-lead-former.php
. CF-9 in action - video. Component Forms Below are some of the most common forms produced by the CF-9 component lead former. Reducing Form Reducing Form with Lock In Stand-off Spread For Spread Form with Lock In Stand-off Lock In Stand-off Form 90 Degree Angle Bend Flush Mount Lock In Form Stand-off Lock In Form Inline
Heller Industries Inc. | https://hellerindustries.com/wp-content/uploads/2018/07/00600-228.pdf
; because none of them are exact drop-in replacements for tin/lead sol- der, all require some process adjustments. The primary difference between most of the new formulations and traditional solder is a higher melting point