Electronics Forum | Tue May 21 16:18:57 EDT 2019 | edhare
Interesting problem. I've seen this before on SMT device leads (see Gold Embrittlement paper at http://www.semlab.com). The AuSn4 IMC is solid at typical reflow temperatures and traps volatiles in the solder joint. One usually cannot crank the ref
Electronics Forum | Wed Oct 24 18:08:02 EDT 2001 | davef
1- DF1: WOW!!! How do people get these cool toys? CB: I am with the University at Buffalo Electronic Packaging Lab. http://www.packaging.buffalo.edu We have pretty much everything that is sold on the market as well as Laser inspection technologies we