Electronics Forum | Thu Aug 15 15:58:12 EDT 2002 | robertnguyen
To whom this may concern, I recently ran into the problem with vias on pads of BGA when place BGA and reflow gas trap on vias escape and result in ball having void greater than 50% of BGA diameter. The BGA pad is measured at 20 mils and the vias mea
Electronics Forum | Fri Aug 16 09:59:49 EDT 2002 | dason_c
We baked the board first and print 2 mil water soluble paste at the BGA location and reflow. Wash and baked before the production run.
Industry News | 2018-10-18 08:32:52.0
How to Prevent Solder Ball and Bridging Defects during the SMT Reflow Process
Industry News | 2010-05-07 16:01:14.0
New this year! The SMTA International Technical Committee invites you to participate in a poster session at SMTA International. Poster sessions are presented on the show floor and are a great way to present current research and results in a concise manner without requiring a technical paper.
· What is the difference between SMT vacuum reflow soldering machine and ordinary reflow soldering machine? · What problems can be solved by smt vacuum reflow soldering machine? · What is the basic principle of vacuum reflow machine? · Ho
SMTnet Express, April 7, 2022, Subscribers: 25,732, Companies: 11,564, Users: 27,174 Effect Of Vacuum Reflow On Solder Joint Voiding In Bumped Components Voids affect the thermal characteristics and mechanical properties of a
SMT Express, Volume 2, Issue No. 3 - from SMTnet.com Volume 2, Issue No. 3 Thursday, March 16, 2000 Featured Article Return to Front Page Curtailing Voids in Fine Pitch Ball Grid Array Solder Joints by Gary Morrison and Kevin Lyne
| http://etasmt.com:9060/te_news_bulletin/2021-08-31/23577.chtml
%. Another key area to be discussed is the maximizing of the unit per hour (UPH) ofthe system while still achieving the void rate reduction < 1
PCB Libraries, Inc. | https://www.pcblibraries.com/Forum/0402-capacitors-under-1-mm-pitch-bga_topic695_post2385.html
and ready for reflow with BGA fanout on one side and capacitor pad on the other side. With capacitors, a small "dimple" (with trapped air) in the pad would not create a void cavity in the lead like they do in BGA via-in-pad