Hello, I had recently a problem of crack between the solder ball (SnPb) and the Ni layer of the PCB pad. We use Electroless Ni/Au technology for PCB. This phenomena is amazing because the crack is very clean (straight) and it creates a space betwee
Electronics Forum | Thu Apr 22 07:51:32 EDT 1999 | Vic Lau
after soldering transistors on a flex circuit (Ni/Au plated), one of the lead lift-up from the pad. under microscope (1,000 X), i find some cracks on the the pad surface. with edx analysis, the surface is mainly nickel. have you ever encounter suc
Industry News | 2011-12-30 23:26:12.0
Nihon Superior has highlighted the effectiveness of Cu and Ni as the essential elements in forming a stable IMC layer in lead-free soldering.
Industry News | 2010-09-02 10:54:09.0
Nihon Superior Co. Ltd., a supplier of advanced soldering materials to the global market, announces that the research it sponsored at the University of Queensland, Australia provided the basis for the paper that earned an ICEP Outstanding Paper Award.
The Morphology Evolution and Voiding of Solder Joints on QFN Central Pads with a Ni/Au Finish SMTnet Express October 19, 2012, Subscribers: 25598, Members: Companies: 9011, Users: 33828 The Morphology Evolution and Voiding of Solder Joints on QFN