On various PCB's after building processes,such as reflow, flowsolder and wash. The soldermask on the PCB's have become discoloured, like a 'marble' effect all along the solder side of the board, it is lighter in contrast than normal, although when ot
Electronics Forum | Mon Oct 24 17:56:57 EDT 2005 | Ali
Hello all: A couple of queries on matte Sn plating: My Application: 2 Reflows in subassembly reflow+ 8 Hr Steam age+ Solderability (Dip and look) for sub assembly to mother board soldering. Queries on Matte Sn: 1- Different plating vendor