Florachem provides cleaning agents including products for defluxing,stencil/misprint cleaning and removal of white residue. We also supply rosin derivatives for manufacture of solder fluxes and pastes
New Equipment | Solder Materials
Kapp Lunar Flux™ is a slurry designed specifically for soldering casted Aluminum, Diecast, Zamak, White Metal and Pot Metal using Alumite™ solder. Residue is electrically conductive and slightly corrosive. Any flux residue should be removed with warm
New Equipment | Solder Materials
Kapp Lunar Flux™ is a white paste for the high temperature soldering of Aluminum and Zinc die cast alloy. It is a reaction-type flux with 70% active ingredients dispersed in alcohol. Kapp Lunar Flux™ has considerable shelf life stability, as the susp
Electronics Forum | Wed Jan 27 19:42:34 EST 1999 | parag palshikar
i am working with the noclean process and getting white residues on the bottomside of the board probably due to the wave soldering flux.i am using a no-clean solder paste and a noclean wave solder flux.The boards passed the accelerated temperature a
Electronics Forum | Thu Jan 28 08:58:10 EST 1999 | Peet
| | i am working with the noclean process and getting white residues on the bottomside of the board probably due to the | | wave soldering flux.i am using a no-clean solder paste and a noclean wave solder flux.The boards passed the accelerated tempe
Industry News | 2011-01-22 00:27:29.0
Design, assembly, soldering, repair, rework, inspection, and materials choice are all variables to be juggled as electronics manufacturers worldwide work with new component types, high speed signals and lead-free technology. To assist them in making the best choices for producing reliable electronics, IPC — Association Connecting Electronics Industries® is holding the IPC Conference on Quality, Reliability and Acceptability for Electronics Manufacturing in Budapest, Hungary, on 22–24 February 2011.
Industry News | 2013-10-21 16:05:48.0
IPC – Association Connecting Electronics Industries® presented Committee Leadership, Special Recognition and Distinguished Committee Service Awards at IPC’s Fall Standards Development Committee Meetings last week in Fort Worth, Texas.
Technical Library | 1999-05-07 10:47:00.0
White residue remaining after cleaning circuit board assemblies can be caused by a variety of chemicals and reactions. Rosin and water-soluble fluxes, circuit board resins and epoxies, component materials and other contamination all contribute to this complex chemistry. This paper discusses many of the sources of the residues that seem to be an ever-increasing occurrence.
Product name: Halogen Free Lead Free Solder Wire Product code: E9650-HF961 Alloy composition: Sn/Ag3.0/Cu0.5 Diameter: 0.2mm, 0.6mm, 0.8mm, 1.0mm, 1.2mm, 1.6mm Packing: 500g/reel, 1kg/reel (10kg/box) Price: Contact us for best price Features:
Heller Industries Inc. | https://hellerindustries.com/fluxless-soldering/
. Using flux, however, has its drawbacks: Flux can outgas during the reflow process creating solder voids. Flux leaves behind a residue which needs to be cleaned post reflow
Surface Mount Technology Association (SMTA) | https://www.smta.org/chapters/chapters_detail.cfm?chapter_id=38
. This information can aid in identifying specific residue sources (e.g. board fabrication, SMT paste flux, waver solder liquid flux, hand solder flux or a completely different flux pen, or bottle or paste flux.) 12:00pm