Electronics Forum: fr4 moisture (56)

HASL, shelf life, IPC standards

Electronics Forum | Wed May 03 16:37:10 EDT 2017 | charliedci

I don't believe there should be any issues with the HASL finish. The issue is how long on the shelf and is a bake out required to remove moisture from PCB, as in any FR4 PCB's that may have had time to absorb moisture.

Re: TCE for Ais

Electronics Forum | Thu Jun 25 11:47:39 EDT 1998 | Steve A

| Hi there, | Does any one know what is TCE for fully wet saturated FR4. I came to know that for Dry FR4 the TCE is about 15-19 PPM �C. Is that true? | | Appreciated for your help. | rgs, | chiakl Chiakl, It looks like you are speaking of what could

Industry News: fr4 moisture (3)

Typical RoHS Issues in PCB Assembly

Industry News | 2018-10-18 10:23:07.0

Typical RoHS Issues in PCB Assembly

Flason Electronic Co.,limited

Krayden Introduces Dow Corning’s 3140 RTV Aerospace Coating

Industry News | 2010-10-20 18:55:44.0

Krayden, Inc., a leading distributor of engineered materials, introduces Dow Corning’s 3140 RTV Aerospace Coating.

Krayden Inc.

Express Newsletter: fr4 moisture (96)

Partner Websites: fr4 moisture (5)


fr4 moisture searches for Companies, Equipment, Machines, Suppliers & Information

Sm t t t t t t t t t t net
  1 2 3 4 5 6 7 8 9 10 Next
Sell Used SMT & Test Equipment

High Precision Fluid Dispensers
Software for SMT

Best Reflow Oven
Best SMT Reflow Oven

World's Best Reflow Oven Customizable for Unique Applications
PCB separator

Original SMT Feeders and spares for Panasonic, Fuji , Yamaha, Juki , Samsung