Electronics Forum | Fri Jul 06 12:39:01 EDT 2007 | blnorman
What's the metallization on the board? We use an immersion tin board and had to increase our profile to successfully solder.
Electronics Forum | Fri Jul 06 12:11:34 EDT 2007 | james
We are starting to see issues with using Kester WS R562 with lead free components. The joints look grainy on almost all of the 0402'2 and other small components. Some of the solder does not solder to the terminations. These are hybrid boards which