Electronics Forum | Fri Feb 15 15:37:35 EST 2019 | emeto
Hello, I have a capacitor that doesn't form intermetallic joint with SAC 305 solder paste.The board is ENIG. Solder melts and forms good intermetallic joint with the PCB finish. However, capacitor can be removed with physical force - it looks like a
Electronics Forum | Fri Nov 09 19:31:43 EST 2007 | yshiau
Thank you to Dave and Scott!! What I'm delaing with is mass production test for small memory cards in volume! The reason I choose Non-operating temperature cycling is so that I can deal with volume. I can throw in quite a few memory cards in chambe
Industry News | 2018-10-18 08:04:17.0
Influences of the solder material for the wave soldering machine soldering quality
SMTnet Express, May 9, 2019, Subscribers: 31,902, Companies: 10,760, Users: 26,083 Cold Ball Pull Test Efficiency for the PCB Pad Cratering Validation with the Ultra Low Loss Dielectric Material Credits: iNEMI (International Electronics