Electronics Forum | Wed Sep 23 00:06:34 EDT 2020 | SMTA-64387098
I have modules that come with a 4 x 2 pin header. The problem is the pins must be oxidized as they do not take solder (no wetting occurring). This occurs whether solder in our wave soldering machine or soldered by hand. I tried cleaning the module i
Electronics Forum | Wed Sep 23 13:56:02 EDT 2020 | emeto
Try to pre-tin the part. This should give you a lot of answers.
Technical Library | 2017-08-17 12:28:30.0
At SMT assembly, flux outgassing/drying is difficult for devices with poor venting channel, and resulted in insufficiently dried/burnt-off flux residue for no-clean process. Examples including: Large low stand-off components such as QFN, LGA Components covered under electromagnetic shield which has either no or few venting holes Components assembled within cavity of board Any other devices with small open space around solder joints
SMT Express, Volume 4, Issue No. 5 - from SMTnet.com Volume 4, Issue No. 5 Thursday, May 23, 2002 Featured Article Return to Front Page Book Review Reviewed by Dave Fish (davef ), Pandion Electronics, Inc. Title: Reflow Soldering
| https://www.eptac.com/blog/everyday-ai-is-here-examples-you-might-not-notice
Everyday AI is Here, Examples You Might Not Notice Looking for solder training standards, manuals, kits, and more? Visit soldertraining.com Training Training Materials Locations Resources Ask Helena
Heller Industries Inc. | https://hellerindustries.com/parts/4670/
4670 - Junction Module- I.D.C 50pin - Obsolete if not in stock Phone 1-973-377-6800 Company About News Events New Equipment Convection Reflow Ovens Reflow Oven MK7 -New