Electronics Forum | Wed Mar 12 15:26:46 EDT 2014 | dan_ems
Hello, in my SMT process I have some problems with the solderability (look like dewetting) on a PCB with finish HASL Lead Free with a composition that is melt at 230 degree Celsius. My oven is with vapor phase and the peak temperature is 230 degre
Electronics Forum | Thu Mar 13 14:12:31 EDT 2014 | davef
You're creating a new alloy on the surface of your board. The alloy will have a melting point determined by the constituent metals of the alloy. Your alloy consists of: * Lead-free HASL solderability protection on the board * Lead-free solder paste *
Heller Industries Inc. | https://hellerindustries.com/recent-searches/
1706 exl 1800exl 1707 mark 5 heller Uf3800 underfill Hac1 manual Vapor phase reflow Rma 204 Reflow soldering on surface mount Reflow qfn Reflow temperature for lead solder Hex250l Training Reflow
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830