Re: Baking of PCB's/Flexes

Electronics Forum | Thu Oct 26 13:56:08 EDT 2000 | ptvianc

Hello: Pre-baking laminates should only be performed:(1) to meet contractual agreements or (2) in response to an actual defect that can be traced to PWB water absortion. Besides the fact that a pre-bake is an enormous process "bottleneck," it also

Pre-bake times and temperature for polyimide boards

Electronics Forum | Wed Jan 12 10:05:20 EST 2005 | Dreamsniper

we are using polyimide boards 6 inches x 7 inches, 2.5mm thick, 12 to 14 layers, for aerospace industries. I am using a long bake of 12 hours at 70'C prior to manufacturing or exposure to elevated reflow and wave soldering temperature. If schedule i

Express Newsletter: prebake pwb (66)

Design and Construction Affects on PWB Reliability

Design and Construction Affects on PWB Reliability SMTnet Express April 26, 2012, Subscribers: 25100, Members: Companies: 8853, Users: 33038 Design and Construction Affects on PWB Reliability First presented at IPC Apex Expo 2012 by: Paul


prebake pwb searches for Companies, Equipment, Machines, Suppliers & Information

Sm t t t t t t t t net
  1 2 3 4 5 6 7 8 Next
SMT feeders

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...
Global manufacturing solutions provider

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.
2024 Eptac IPC Certification Training Schedule

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
SMT Spare Parts

Private label coffee for your company - your logo & message on each bag!