Electronics Forum: root cause for lifted pads (10)

BGA Voiding for RoHS

Electronics Forum | Mon Nov 09 07:21:02 EST 2009 | CL

Good Morning, I have seen many posts regarding BGA voiding being excessive and what can be done to better the condition. I have a customer that has an assembly that we have had a diufficult time with. We have spent a lot of time debugging the proces

Optimal Speed for Universal Chip Shooters

Electronics Forum | Wed Jun 11 16:30:33 EDT 2003 | T.Vick

You have received some great feedback so far. I would like to summarize and add a few points regarding maintenance. You should start (as recommended already) by verifying your component library data. Using the default values from the master library i

Industry News: root cause for lifted pads (5)

How to Prevent the Tombstone and Open Defects during the SMT Reflow Process

Industry News | 2018-10-18 08:14:11.0

How to Prevent the Tombstone and Open Defects during the SMT Reflow Process

Flason Electronic Co.,limited

Koh Young SPI Dispenses Solder Paste for 0402M (01005) Microchips

Industry News | 2018-09-04 10:25:16.0

Seoul, South Korea – Flexible SMT production has entered into a new dimension. Koh Young Technology’s 3D SPI (Solder Paste Inspection) system has now expanded its solution to perform complex dispensing. Koh Young highlighted the latest innovations, including its new high-precision, integrated dispenser for the KY8030-3 3D SPI in Stand 1F45 at NEPCON South China, which occurred August 28-30, 2018 in Shenzhen, China.

Koh Young America, Inc.

Express Newsletter: root cause for lifted pads (373)

Partner Websites: root cause for lifted pads (20)

Identifying and Correcting Solder Bridge Defects | Imagineering, Inc.

Imagineering, Inc. | https://www.pcbnet.com/blog/identifying-and-correcting-solder-bridge-defects/

. Unfortunately, there are numerous causes that can produce solder bridging. To produce as quickly and efficiently as possible, finding the root cause of this defect is critical

Imagineering, Inc.

How to Prevent Non-Wetting Defect during the SMT Reflow Process-SMT Technical-Reflow oven,SMT Reflow

| http://etasmt.com/cc?ID=te_news_industry,24564&url=_print

. Dewetting directly impacts the quality of solder joints. Root Cause Analysis The PCB pads or the component‘s pins are oxidized. An oxidation layer prevents contact between the solder and the surface plating layer