New SMT Equipment: salt residues (5)

Kapp Copper-Bond Flux - High Temperature Soldering Flux

Kapp Copper-Bond Flux - High Temperature Soldering Flux

New Equipment | Solder Materials

Kapp Copper-Bond Flux™ has been designed for high temperature soldering of all common metals except Aluminum. Kapp Copper-Bond Flux™ is an activated liquid flux containing a mixture of inorganic salts in water, with approximately 50% active ingredien

Kapp Alloy & Wire, Inc

Kapp Comet Flux - Low Temperature Soldering Flux

Kapp Comet Flux - Low Temperature Soldering Flux

New Equipment | Solder Materials

Kapp Comet Flux™ has been designed specifically for soldering all common metals except Aluminum. Kapp Comet Flux™ is an activated liquid flux, a mixture of inorganic salts in water, with approximately 35-40% active ingredients. Highly recommended f

Kapp Alloy & Wire, Inc

Electronics Forum: salt residues (36)

White residues

Electronics Forum | Mon Apr 29 09:54:46 EDT 2002 | davef

MadReindeer If this white residue is salt, * Why do you say is the presence of it 'not dangerous it only looking bad'? Don't salts sometimes go into solution with moisture on the board from humidity in the air and form cathodic plating shorts betw

White residues

Electronics Forum | Mon Apr 29 04:57:28 EDT 2002 | madreindeer

Hi, That is very common in WS pastes.It is white residue (Salt) Usually it�s not dangerous it only looking bad. I think best way would be contact your paste supplier and they should know what would take a stain off if not, change supplier. There i

Industry News: salt residues (4)

SMTA Intermountain Chapter to Hold Annual Technical Symposium

Industry News | 2013-09-10 12:18:26.0

The Surface Mount Technology Association (SMTA)'s Intermountain Chapter will hold its annual technical symposium on September 19 at the University of Utah in the Warnock Engineering Building, Salt Lake City, Utah.

Surface Mount Technology Association (SMTA)

How To Set Profile In SMT Reflow Oven

Industry News | 2018-10-18 09:37:27.0

How To Set Profile In SMT Reflow Oven

Flason Electronic Co.,limited

Technical Library: salt residues (1)

Influence of Salt Residues on BGA Head on Pillow (Hip)

Technical Library | 2016-05-26 15:07:36.0

The oxide layers are known as wetting inhibitors in component and PCB metallizations. The oxide acts as barrier that prevent the tin diffusion from happening. Besides, in corrosion studies, the role of salt residues -with Cl ion- on some metals is known as being promoters of oxidation or corrosion. On the other hand, most of corrosion studies with tin metallization are focused mainly on the corrosion resistance of tin alloys, but little has been done respecting to the influence of salts on tin metallization wetting. In this paper, a series of experiments was carried over to know the influence of specifically NaCl on BGA wetting given Head in Pillow (HiP) as result.

Continental Corporation

Videos: salt residues (2)

Nu/Clean Aqua Batch

Nu/Clean Aqua Batch

Videos

See the Nu/Clean Aqua Batch Aqueous Batch Cleaner in operation! Quick, quiet, close loop cleaning at a great price! For technical specifications, visit our website www.TechnicalDev.com.

Technical Devices Company

Nu/Clean Aqua Batch

Nu/Clean Aqua Batch

Videos

See the Nu/Clean Aqua Batch Aqueous Batch Cleaner in operation! Quick, quiet, close loop cleaning at a great price! For technical specifications, visit our website www.TechnicalDev.com.

Technical Devices Company

Express Newsletter: salt residues (168)

SMTnet Express - May 26, 2016

SMTnet Express, May 26, 2016, Subscribers: 24,776, Companies: 14,803, Users: 40,361 Influence of Salt Residues on BGA Head on Pillow (Hip) J. Servin, P. Gomez, M. Dominguez, A. Aragon; Continental Corporation The oxide layers are known as wetting

Partner Websites: salt residues (4)


salt residues searches for Companies, Equipment, Machines, Suppliers & Information

Sm t t t t t t t t t t net
  1 2 3 4 5 6 7 8 9 10 Next