Electronics Forum | Tue Jan 14 10:48:07 EST 2020 | dontfeedphils
I've worked with these quite a bit in the past as well. As the previous poster mentioned, we ran either 4/5 mil thick stencil with a pretty standard RTS profile in a 10 zone convention oven without issue.
Electronics Forum | Wed Jan 15 12:10:22 EST 2020 | emeto
Avillaro, I don't have hands on experience with Vapor Phase equipment, but my guess is that it will work better for thick boards like yours. Trying another chemistry is a logical move. May be it is worth trying the fixture for connector flatness as n
Industry News | 2018-10-18 10:18:58.0
Case study: How to Create a Reflow Profile for a 16-layer, 2mm Thickness PCB with a High Density SMT Connector?
Connector Models - Are They Any Good? Connector Models - Are They Any Good? by: Jim Nadolny, Leon Wu; Samtec, Inc. Channel simulations are only as accurate as the models used to develop them. While we have seen much effort placed on printed