Electronics Forum: sn90pb10 (5)

BGA ball and PCB pad

Electronics Forum | Fri Feb 13 11:46:23 EST 2004 | Jack

Is your customer trying to reduce voiding? If the device is using Sn90 / Pb10 and the paste is Sn63/Pb37 the board will melt first. However, if both solders are 183C eutectic, it's a tossup? PCB design, copper weight, bga type (pbga, micro bga, Tbg

0402 tombstoning and dewetting on QFP256 trade-off

Electronics Forum | Fri Mar 06 02:47:15 EST 2009 | lococost

Have you tried higher peaktemp? I saw the QFP is sn90pb10, This has a liquidus of 268 - 302 C. A good paste should be able to handle 230C (or more), of course you would need to check your other components peak temp.


sn90pb10 searches for Companies, Equipment, Machines, Suppliers & Information

Sm t net
  1  
Voidless Reflow Soldering

High Throughput Reflow Oven
pressure curing ovens

High Precision Fluid Dispensers
convection smt reflow ovens

World's Best Reflow Oven Customizable for Unique Applications
Fully Automatic BGA Rework Station

SMT & PCB Equipment - MPM, DEK, Heller, Europlacer and more...