Electronics Forum | Mon Jun 14 17:21:31 EDT 2004 | russ
How old are these parts? Sn/Ni plating is very succeptable to age and everything else. They are possibly tarnished. Also, what is your peak temp in reflow? It takes about 225 230 C to get good wetting to the underlying nickel. Russ
Electronics Forum | Mon Apr 25 21:52:58 EDT 2005 | KEN
I wonder if yor customer means wrong "flux"? Your not solderng to gold. Your soldering to Nickle. The gold is disolved and dispersed. Your joint strength comes from the SnNi intermetalic.