Industry Directory | Manufacturer
Integran's hard nickel blanks for SMT solder stencils can be laser cut into the highest performance solder stencils on the market. Quality is underpinned by Integran's strong analytical capabilities.
Industry Directory | Manufacturer
Integran makes nanocrystalline nickel SMT solder stencil blanks that are subsequently laser cut into the high durability and very precise stencils. We make 500-1000 a month of 22.5" x 24" foils.
New Equipment | Education/Training
Failure Analysis Techniques for Electronics provides an overview of the characterization methods available at ACI Technologies, Inc. for determining the causes of failure in electronics devices. This publication will assist the reader in making inf
New Equipment | Solder Paste Stencils
SMT Framed Stencils are laser cut solder paste stencils designed to work on SMT printing machines. These laser cut stencils are permanently glued into a frame. These framed stencils are are designed for highly repeatable continuous operation in volum
Electronics Forum | Wed May 11 13:27:30 EDT 2005 | Sam Ho
i want to know which type of solder paste and reflow profile can support the solder pad with nickel but not covered gold on the pcb.
Electronics Forum | Wed May 11 13:50:30 EDT 2005 | russ
I would contact your paste supplier, bare nickel can be impossible to wet to. How oxidized is it?
Used SMT Equipment | Soldering - Reflow
Intelligent hot air lead-free reflow Oven with six heating-zones TN360C Instruction: 1: Heating system: TN360C adopts high effective nickel-chromium heating tube with advanced technology and Long life service. The hot-air circle system wh
Industry News | 2003-05-19 10:06:43.0
The PCB is available with a maximum panel size of 406-by-460mm and a minimum board thickness of 0.8mm.
Industry News | 2003-03-21 08:12:24.0
Tecan reckons it is consistently producing what may be regarded as the most efficient stencils in the world today.
Parts & Supplies | Circuit Board Assembly Products
1). 1+C+1 HDI, buried/blind L1-L5/L5-L8 vias. 2). FR-4 Material, 1 oz weight. 3). 8 layer, 1.6mm thick. 4). 4/4 mils track and space 5). Min.drill 0.1mm 6). Green solder mask/ white silkscreen 7). Immersion gold over nickel
Technical Library | 2019-06-04 10:19:46.0
Interconnection technology relies very heavily on the ability of the conductors on a printed wiring assembly to maintain reliable signal integrity. Harsh environmental factors can precipitate a loss of conductivity due to oxidation and corrosion. Connections are typically soldered or inserted using pressure fitted connectors to obtain enough surface contact to meet the electrical conductivity requirements. In pressure contacts, surface integrity is especially critical where the abrasive effects of retraction and insertion can wear off the metallic finish from the contact area. This can expose the underlying copper or nickel and lead to increased resistance at the contact points. These types of conductors are frequently found in card edge connectors where the terminations are plated with a layer of nickel and gold (frequently referred to as gold fingers). A hard gold is typically used containing very small amounts of nickel and cobalt to increase the wear resistance.
Technical Library | 2019-06-07 14:49:54.0
ACI Technologies was contacted in regards to poor solder joint reliability. The customer submitted an assembly that was exhibiting intermittent opens at multiple locations on a ball grid array (BGA) component. The assembly’s functionality did not survive international shipping, essentially shock and vibration failures, immediately making the quality of the solder joints suspect. The customer was asked about the contract manufacturer and the reflow oven profile as well as the solder paste and surface finish used. The ACI engineering staff evaluated the contract manufacturer’s technique and determined that they were competent in the methods they used for placing thermocouples in the proper locations and developing the reflow oven profile. The surface finish was unusual, but not unheard of, in that it was hard gold over hard nickel, rather than electroless nickel immersion gold (ENIG). The customer was able to supply boundary scan testing data which showed a diagonal row of troublesome BGA pins.
ACI Technologies Inc. (ACI) is a scientific research corporation dedicated to the advancement of electronics manufacturing processes and materials for The Department of Defense and industry. This video provides an overview of our commercial service
This is video shows how to print a PCB using a prototype foil only stencil. The SMT prototype stencil (www.soldertools.net) is made from a high nickel content material able to offer repeatable high precision apertures. The steps of alignment, printin
Events Calendar | Tue Jan 23 00:00:00 EST 2018 - Tue Jan 23 00:00:00 EST 2018 | New Milford, Connecticut USA
FREE Webinar: Eliminate Circuit Board Problems and Failure Modes
Events Calendar | Wed Mar 18 00:00:00 EDT 2020 - Wed Mar 18 00:00:00 EDT 2020 | College Park, Maryland USA
CALCE Reliability Science Symposium - Spring 2020
Career Center | NORTHRIDGE, California USA | Engineering
EDUCATION BS Electronics and Communication Engineering Gujarat University MS Electrical Engineering California State University, Northridge ACADAMIC PROJECT Fabrication and Characterization of Silicon Carbide (SiC) MESFE
SMTnet Express, November 6, 2014, Subscribers: 23500, Members: Companies: 14091, Users: 37109 Effect of Process Variations on Solder Joint Reliability for Nickel-based Surface Finishes Hugh Roberts, Sven Lamprecht, Gustavo Ramos, Christian Sebald
Wire Bonding and Soldering on Enepig and Enep Surface Finishes with Pure Pd-Layers SMTnet Express October 11, 2012, Subscribers: 25550, Members: Companies: 9005, Users: 33789 Wire Bonding and Soldering on Enepig and Enep Surface Finishes with Pure
Heller Industries Inc. | https://hellerindustries.com/parts/589869/
589869 - Lead Screw, CLS, Nickel Plate Phone 1-973-377-6800 Company About News Events New Equipment Convection Reflow Ovens Reflow Oven MK7 -New
ASYMTEK Products | Nordson Electronics Solutions | https://www.nordson.com/en/divisions/efd/resource-center/solder-selection-guide
Monel Nichrome Nickel Nickel Iron / Alloy42 Nickel Silver Palladium Platinum Silver Solder Plated Stainless Steel Tin Titanium Non-solderable Zinc Key Recommended Alloy Specific (contact EFD