Electronics Forum | Mon Aug 17 02:50:44 EDT 1998 | Bob Willis
| Have an SRT w/preheat, 18 layer board all copper, 456 BGA needs to be removed and replaced. The manufacturer is Chip Express and during reflow it warps up or down. Causing either opens or shorts on the corners. I was using gel flux with multiple
Electronics Forum | Fri Jul 30 17:13:30 EDT 1999 | Dave F
| | | Looking for solder paste specification limits which have reliability data to support them. Currently, we are looking to define the min/max volume necessary to ensure a good joint on CBGA, PBGA, and Micro-BGA's. Any information will be greatly
Technical Library | 2019-05-15 22:26:02.0
As the demand for higher routing density and transfer speed increases, Via-In-Pad Plated Over (VIPPO) has become more common on high-end telecommunications products. The interactions of VIPPO with other features used on a PCB such as the traditional dog-bone pad design could induce solder joints to separate during the second and thereafter reflows. The failure has been successfully reproduced, and the typical failure signature of a joint separation has been summarized.To better understand the solder separation mechanism, this study focuses on designing a test vehicle to address the following three perspectives: PCB material properties, specifically the Z-direction or out-of-plane Coefficient of Thermal Expansion (CTE); PCB thickness and back drill depth; and quantification of the driving force magnitude beyond which the separation is due to occur.
SMTnet Express, May 16, 2019, Subscribers: 31,918, Companies: 10,765, Users: 26,116 Transient Solder Separation of BGA Solder Joint During Second Reflow Cycle Credits: Cisco Systems, Inc. As the demand for higher routing density and transfer speed
SMT Express, Volume 2, Issue No. 3 - from SMTnet.com Volume 2, Issue No. 3 Thursday, March 16, 2000 Featured Article Return to Front Page Curtailing Voids in Fine Pitch Ball Grid Array Solder Joints by Gary Morrison and Kevin Lyne
Heller 公司 | http://hellerindustries.com.cn/Vacuum-Void-Reduction-Reflow.pdf
phases in the Pb-free microstructure. RESULTS Solder Joint Void Characterization The factory x-ray inspection on the conventional or standard SMT (STD SMT) reflow assembly revealed substantial void content in the BGA solder joints of both components. The x
Surface Mount Technology Association (SMTA) | https://www.smta.org/knowledge/journal.cfm
SOLDER JOINT RELIABILITY OF Sn-Ag-Cu BGA COMPONENTS ATTACHED WITH EUTECTIC Pb-Sn SOLDER PASTE Fay Hua et al. Abstract 2002 15-4 IMPACT OF COMPONENT TERMINAL FINISH ON THE RELIABILITY OF Pb-FREE SOLDER JOINTS Gregory Henshall et al. Abstract 15-4 EFFECT OF