SMTnet Express, November 19, 2017, Subscribers: 30,938, Companies: 10,768, Users: 23,942 To Quantify a Wetting Balance Curve Frank Xu Ph.D., Robert Farrell, Rita Mohanty Ph.D.; Enthone Wetting balance testing has been an industry standard
ASYMTEK Products | Nordson Electronics Solutions | https://www.nordson.com/en/divisions/march/about-us/news/new-march-plasma-treatment-system-with-2-meter-depth-for-improved-manufacturing
. Also included are configurable plasma cells with high flux electrodes and direct gas injection for uniform gas flow. Besides catheters, PROGENY systems can plasma-treat other products with part surfaces up to 2 m long and 50 cm wide that need better wetting, coating, and adhesion
Heller Industries Inc. | https://hellerindustries.com/wp-content/uploads/2018/07/leadfree.pdf
Procured test board with bare copper pads protected with OSP. (Future testing to be run with HASL Lead Free Pads) ♦ Tested 2 pastes: ♦ 96.5% Sn/3.5% Ag with RMA flux melt point 221