Electronics Forum | Fri Jan 17 11:40:36 EST 2020 | davef
Try preheating the connectors
Electronics Forum | Thu Jan 16 05:10:46 EST 2020 | soupy
Hej, we have some connectors placed on our PCB. 2*30legs 0.5 After reflow we detect lifted legs in the AOI. Always on the outer corners. Is this something ye have experienced? And any possible solutions? Stuff we have tried: Checking the cop
Electronics Forum | Fri Jan 17 02:29:59 EST 2020 | soupy
Thanks Dave, We have avoided rotating the board as it is so long but we will test. Maybe we will to try screen it in one direction and then rotate it before the oven. We have the maximum solder we can get there at the moment. The reflow engineer
Electronics Forum | Thu Jan 16 10:07:12 EST 2020 | davef
Hej back at ya Your connectors could be warping during reflow. Find out by putting a connector on a hot plate and increasing the temperature. If so, you might get away with a simple fix of rotating the board 90* on your reflow oven conveyor. If you
Electronics Forum | Wed Oct 29 23:07:42 EDT 2014 | rajz
Help Needed. I face a solder bridging issue on solder mask define pad at edge only for nexlev connector . The pad design such as smd at four corner only. The bridging happen on signal to ground pin only. Current stencil we use 22 round with 6 mils s
Electronics Forum | Mon Jan 16 00:47:47 EST 2012 | ngineer
I have two new quad feeder bases and feeders (my machine came with none to start, and I can't find any electrical information on them. I have 4 pins at the each end (total of 4 connectors. And are in a 4 pin connector which looks identical to a sta
Electronics Forum | Tue Nov 07 08:09:19 EST 2000 | adam
WE are using press fit connnectors on a range of boards, one of which is posing me a few process questions . The Machine is a fully automatic machine. The problem is intermittent and I can't seem to put a finger on it. An array of connectors ( consi
Electronics Forum | Tue May 28 21:00:59 EDT 2002 | davef
That is the rub here, isn�t it? For those posting, it�s easier [but much slower] to start a new thread than to search the archives. [And posters could view their issue so unique and novel that it could never have been discussed several years earlie
Electronics Forum | Tue Mar 09 19:40:47 EST 2004 | Vijay
The shorts happen at corner of the BGA. The PCB thickness is 1.6mm, It is a PC motherboard with all thru hole connectors mounted on.The preheating is done using IR heater and the temp is 120-160 for about 70-80 sec.I am using ERSA IR550A
Electronics Forum | Tue Mar 09 19:40:55 EST 2004 | Vijay
The shorts happen at corner of the BGA. The PCB thickness is 1.6mm, It is a PC motherboard with all thru hole connectors mounted on.The preheating is done using IR heater and the temp is 120-160 for about 70-80 sec.I am using ERSA IR550A