PCB immersion silver discolouration

Electronics Forum | Sat Sep 20 07:11:28 EDT 2008 | Sean

Hello All, I used to hear that PCB with immersion silver finishing, its non component location pads, tend to be discolour (Yellowish) after went through heat cycle, such as reflow oven. However, if the component solderbility on the PCB is OK, can w

PCB immersion silver discolouration

Electronics Forum | Tue Sep 23 10:06:29 EDT 2008 | Sean

Hello Vlad, Davef, Your valuable inputs are much appreciated. Many thanks, Sean.

PCB immersion silver discolouration

Electronics Forum | Sun Sep 21 10:55:52 EDT 2008 | vladig

As long as the surface is solderable, you should be fine. Silver tarnish a well0-known thing. Make sure, though, there is no sulfur (S) "around". Regards, Vlad

PCB immersion silver discolouration

Electronics Forum | Mon Sep 22 15:32:20 EDT 2008 | davef

We see this fairly often. It doesn't affect solderability. Our analysis makes us think this coloration is copper. The reason copper appears on the surface may be that heat cycles increase the thinness and porosity of the immersion silver [IAg] coatin

Immersion silver life span

Electronics Forum | Mon Apr 18 20:44:30 EDT 2005 | davef

Charly: Why do you "need to bake the PCb due to moisture issue", if you're not going to use the board? Why bake the board, just to put it back in storage, absorb moisture, and require baking again?

imm. silver

Electronics Forum | Fri Aug 30 16:25:21 EDT 2002 | davef

Imm silver holds-up to multiple thermal cycles very well. The things, we guess, are happening to make imm silver tough to solder after heating and sitting are: * Oxidation of the silver. * Reduction of the co-deposited organic anti-tarnish [used in

Re: silver finishes on pcbs

Electronics Forum | Thu Dec 14 10:14:04 EST 2000 | PeteB

Jacqueline, Asuming you mean immersion silver: Advantages - Very flat finish compared to HASL, more easily solderable than bare copper with OSP and more process tolerant than this in our experience, reasonable shelf life, cheaper than immersion gol

Immersion silver life span

Electronics Forum | Wed Apr 13 05:48:52 EDT 2005 | charly

hi' i need advise on immersion silver PCb shelf life. 1) what is the shelf life for Immersion silver PCB? 2) iF PCB expire, can we bake the immersion PCB? what temp & duration? 3) How long can we keep the pCB again after rebaking? (with vacuum seal)

Immersion silver life span

Electronics Forum | Fri Apr 15 05:52:20 EDT 2005 | charly

hi Jon, does it mean the protective layer is coated after the immersion silver process? if we need to bake the PCb due to moisture issue, then we can not hold the pCB long due to the missing protective layer even with vacuum seal environment

Immersion silver life span

Electronics Forum | Thu Apr 14 06:00:01 EDT 2005 | bryan

The shelf life of immersion silver is 6 to 12 months in good storage conditions. The finish is usually coated with a protective layer that inhibits oxidation (like with copper OSP). Care must be taken when handling the boards as the protective la

  1 2 3 4 5 6 7 8 9 10 Next

immersion silver pcb storage searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830