Electronics Forum | Wed Mar 03 17:09:55 EST 1999 | Tom Reilly
We have recently had problems with bare boards coming in too thick. I would like to know how to properly specify the minimum and maximum thickness using the 13949F and IPC 4101 specs. (We currently use "MATERIAL: GFN 0620 C1/C1 A2A per MIL - P - 1394
Electronics Forum | Wed Mar 03 20:20:30 EST 1999 | Earl Moon
| We have recently had problems with bare boards coming in too thick. I would like to know how to properly specify the minimum and maximum thickness using the 13949F and IPC 4101 specs. (We currently use "MATERIAL: GFN 0620 C1/C1 A2A per MIL - P - 13
Electronics Forum | Tue Feb 12 10:33:45 EST 2002 | davef
IPC-4101 - Specification For Base Materials For Rigid And Multilayer Boards replaces MIL-P-13949 - Plastic Sheet, Laminated, Copper-Clad (For Printed Wiring) Taking a broader look, there are many �Obsolete MIL Document To Commercial Document� replac
Electronics Forum | Sun Aug 08 11:15:32 EDT 1999 | Earl Moon
| | Mike, | | | | Got your message and those of others concerning PCB fab supplier evaluation and qualification check lists, etc. I have a severe problem here in WI as I can hardly access the internet, and when I do it is cut off abruptly for no goo