Electronics Forum | Tue Aug 30 09:24:08 EDT 2005 | Slaine
we manufacture a range of ceramic parts that have silver termination,there is already a small leaching problem (absorption of the termination by the solder in liquid form)with Sn62 that we live with, having to implement unleaded solder they are norma
Electronics Forum | Tue Aug 30 12:49:59 EDT 2005 | Ted
Slaine, We use a Pd/Ag thickfilm paste. Because of the leaching we had to start using solder pastes that have silver in it. For RoHS, we are using a solder paste with an alloy of Sn95/Ag05. We also have to double print the thickfilm pastes. I h
Electronics Forum | Wed Oct 10 14:21:04 EDT 2007 | petep
We have done the Green Framed Stencils for an added $50.00 per, then got smart and went to green polyester on RoHS / Lead Free Stencils at no added cost. Dedicated Stencil blades and holders green of course) as well as Green Static mats on dedicated