Electronics Forum | Fri Apr 02 01:05:34 EST 2004 | Grant Petty
Hi, Thanks for the info. How clean can wave soldering get? We are looking at a carrier that masks off most of the board when we run it through the wave, so hopefully this works. Regards, Grant Blackmagic Design
Electronics Forum | Wed Mar 24 08:37:32 EST 2004 | steveliu
Hi, Guys, Can anybody tell me what kind of reflow profile is best for a no clean solder paste: Ramp-Soak-Spike or Ramp-to Spike? The paste we are using is AIM 293DX2B. Thanks a lot.
Electronics Forum | Wed Mar 24 16:28:06 EST 2004 | davef
No-clean flux residues can be either cleanable or not cleanable. The not cleanable type leave a milky white residue on the solder connection after suitable soaking in water. Your flux supplier will have suggestions on the appropriate flux.
Electronics Forum | Tue Mar 30 22:30:06 EST 2004 | davef
Tony First, drying at 125*C for an hour is not going to do much drying. Heck, those boards are barely warm to the touch. Second, tell us about: * Pitch of your uBGA * Solder paste flux * Cleaning process and agents
Electronics Forum | Wed Mar 31 21:27:00 EST 2004 | marcowong
Dear Darren, Please provide more information of your machine, selling price and where it is at the moment. If it is not in Penang malaysia, please also let us know the transportation cost too. Thank you.
Electronics Forum | Thu Apr 01 08:44:58 EST 2004 | pjc
Be smart, be skeptical and be educated on the machines you are looking at. If you are going to do business with someone you don�t know, check them out. Ask others in your region and get at least ten customer references from them.
Electronics Forum | Mon Apr 05 10:37:49 EDT 2004 | Verm.
A customer of ours has requested information on components tested using a torque meter. We have the facility to do this but it is a very uncommon practise. Does anyone else do this during their manufacturing process and if so is there a procedure to
Electronics Forum | Wed Apr 07 20:58:50 EDT 2004 | davef
There's a variety of reports like you see on the net. Here's one: http://www.buscom.com/chem/C137N.html
Electronics Forum | Sat Apr 10 11:47:16 EDT 2004 | mskler
Hi all, When we are producing A gold Plated PCB Then the Prob Of Dry soldering is coming Profile temps are 130, 150, 180,and 220 top & 215 bottom.Then what are the other causes or Precautions may be taken.
Electronics Forum | Sun Apr 11 14:35:25 EDT 2004 | davef
Please: * Describe the color and texture of the dry solder connection on the board. * Tell us the thickness of the gold and nickle plating on the board pads. * Inform us about the width and scope of the problem.