Electronics Forum: cleaning prior (Page 2 of 21)

Flux residue cleaning procedure

Electronics Forum | Sun Oct 29 22:41:29 EST 2006 | hanocete

We have a current problem on our packages after we bake it for 24 hrs prior BGA rework. Flux or white residues found on the connector leads and terminals that cause not contact problems during mating. Could you help us how to clean the fluxes properl

Flux residue cleaning procedure

Electronics Forum | Tue Oct 31 01:32:47 EST 2006 | hanocete

thanks for your reply, actually we bake the PCB assembly prior the rework because the package was exposed for quite some time already. The baking time was 24hrs @ 125 deg.C. We notice that there were flux residues on the connectors after the baking.

Water cleaning and Moisture Entrapment

Electronics Forum | Mon Jan 12 02:56:42 EST 2009 | sachu_70

Hi Bill, You should try pre-baking any such old devices prior to using on SMT Reflow. Refering to MSL-type3 guidelines could help in your case.

Foam fluxer maintenance, storage and cleaning

Electronics Forum | Mon Nov 09 09:44:22 EST 2015 | davef

Purpose. This describes setting-up a wave soldering system set-up for a new assembly design or checking a wave solder machine operation with a test board. Applicability. To be used for new design printed circuit assembles and during machine accept

What is the best method for cleaning PCBs

Electronics Forum | Sat Aug 27 09:17:17 EDT 2011 | davef

We assume from the way you wrote the posting that we're talking about bare boards delivered from your fabricator. If that's the case, the best way to clean these boards is to tell your supplier to clean the boards before sending them to you. You shou

Aluminum wire bonding on ENEPIG plated PCB

Electronics Forum | Tue Sep 10 10:42:36 EDT 2013 | capse

Plasma cleaning is used extensively to clean surfaces prior to wire bonding.

Cleaning Reworked BGA's.

Electronics Forum | Tue Aug 02 21:37:21 EDT 2005 | davef

Are we talking: * BGA that you've reballed and want to clean prior to attachment to a circuit board? * BGA that you've attached to a circuit board after correcting something or other? ... and we're talking a water soluble flux or what?

Stencil cleanliness and inspection

Electronics Forum | Tue Jun 05 16:40:46 EDT 2001 | kerryn

Thanks Phil. However, my objective is to identify stencils that are not 100% clean prior to sending to inventory. I want to catch it before the solder paste has a chance to dry and harden in the apertures. Kerry

Re: Clean before conformal coating?

Electronics Forum | Fri Jan 05 09:23:10 EST 2001 | Brian Toleno

While there may not be any specific requirement to cleaning prior to coating, cleaning an assembly prior to coating will only serve to increase the reliability and integrity of the coating. Some residues from low-solids fluxes can interact with conf

Clean before conformal coating?

Electronics Forum | Thu Jan 04 17:26:17 EST 2001 | Cory

We're going to begin conformal coating a few of our assemblies as required by our customer. We're using Kester No clean paste and will use cotton gloves to keep the boards clean while handling. My question is: Do we need to clean the boards prior to


cleaning prior searches for Companies, Equipment, Machines, Suppliers & Information

Circuit Board, PCB Assembly & electronics manufacturing service provider

Reflow Soldering 101 Training Course
Solder Paste Dispensing

Software for SMT placement & AOI - Free Download.
best pcb reflow oven

Training online, at your facility, or at one of our worldwide training centers"
SMTAI 2024 - SMTA International

High Throughput Reflow Oven