Gold plating thickness on gold finger

Electronics Forum | Thu Oct 07 20:34:48 EDT 1999 | Tony Huang

Hi, Does anybody know what is the minimum gold plating thickness on the PCB goldfinger required by the industrial specifications - IPC, Bellcore, etc. Where can I find the information? Appreciate for the help! Thanks, Tony

looking for HASL TIN thickness specification

Electronics Forum | Tue Sep 02 22:21:26 EDT 2008 | davef

IPC-6012 Table 3-2. States "Fused tin-lead or solder coat - Coverage and Solderable". The lack of any specific dimension criteria doesn't make this any less a requirement. There must be complete coverage of solder on the land, and it must be wettable

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Wed May 27 21:05:30 EDT 1998 | Steve Gregory

Hey yooze guys! Enough of the jokes between you and Earl (GRIN), let's get back to the topic...well, okay... you can tell a few more...(but good ones, 'kay?) Anyhoo...I'm not sure if ya'll are on the IPC Technet list or not, I've not seen any posts f

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Tue May 26 14:50:07 EDT 1998 | Dave F

| | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and sol

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Tue May 26 20:18:09 EDT 1998 | Justin Medernach

| | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Tue May 26 21:27:33 EDT 1998 | Earl Moon

| | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered a

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Wed May 27 11:19:34 EDT 1998 | Earl Moon

| | | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Thu May 28 05:43:33 EDT 1998 | Earl Moon

| Hey yooze guys! | Enough of the jokes between you and Earl (GRIN), let's get back to the topic...well, okay... you can tell a few more...(but good ones, 'kay?) | Anyhoo...I'm not sure if ya'll are on the IPC Technet list or not, I've not seen any p

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Thu May 28 07:25:58 EDT 1998 | Earl Moon

| Hey yooze guys! | Enough of the jokes between you and Earl (GRIN), let's get back to the topic...well, okay... you can tell a few more...(but good ones, 'kay?) | Anyhoo...I'm not sure if ya'll are on the IPC Technet list or not, I've not seen any p

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Tue May 26 15:27:36 EDT 1998 | Dave F

| | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and s


minimum hasl thickness ipc searches for Companies, Equipment, Machines, Suppliers & Information

Association Connecting Electronics Industries (IPC)
Association Connecting Electronics Industries (IPC)

IPC is the trade association for the printed wiring board and electronics assembly industries.

Training Provider / Events Organizer / Association / Non-Profit

3000 Lakeside Drive, 309 S
Bannockburn, IL USA

Phone: 847-615-7100