Electronics Forum | Mon Nov 19 20:15:39 EST 2001 | davef
Now, that is one thickass board!!! The rant first: If our �board supplier changed our board surface finish on� anything without our approval, the board supplier would be an �X�. Life has enough surprises. And of all the flat finishes available, h
Electronics Forum | Wed May 22 08:43:40 EDT 2002 | pjc
I have experience cleaning NC for military boards. The reason for cleaning the NC is due to conformal coating requirements. Zestron Vigon A200 and Atron AC 100, as well as Petroferm Hydrex DX have both been effective at cleaning Alpha UP78 NC paste.
Electronics Forum | Thu Jul 25 21:49:55 EDT 2002 | davef
Consider: * Quitting the coating business all together and using a coating service supplier, like: Thermospray Co 800-952-5838 Mike Moninger; Advanced Coating 800-722-1444; Epsco 108 W. 37th St Boise Idaho 83714 (208)389-2000 * Buying a programmable
Electronics Forum | Wed Oct 02 09:36:10 EDT 2002 | scottefiske
Dragon, Was recently responsible for No Clean Process/Material evaluation and implementation project. Shop was 100% Water soluble facility. Several Top Paste manufacturers were invited to participate. (3) were evaluated. All key variables were identi
Electronics Forum | Wed Oct 23 16:56:03 EDT 2002 | mikestringer
Hi Marc I too have been using a fully synthetic Motor oil on Heller reflow ovens for a number of years. In our case Mobil 1 5W-50. We have a field failure problem with some 1% resistors under conformal coating where sulphates are dissolving the si
Electronics Forum | Fri Jul 04 21:09:04 EDT 2003 | ramanandkini
I have a CEM-1 PCB board with 35 microns copper. This is PCB is finished with SMOBC+HALS. We do solder SMT LEDs, but till date we do not have problems that you have listed. The LEDs are good & bright. It even passed high & low temp cycle tests (-40 t
Electronics Forum | Thu Sep 11 15:23:31 EDT 2003 | Peter L.
I have come across a rash of failed assemblies that have 0805 capacitors and resistors, bottom side glued, wave soldered and washed. Trouble shooter reported touching up the solder joints on a few areas and the boards would pass test. I had a look a
Electronics Forum | Mon Sep 22 23:27:09 EDT 2003 | severs
By "hacking" do you mean altering the performance of the board or something else? This reminds me of something I saw a while back. Better termed counterfeiting than hacking, it may have some relevance to what your friend is trying to do. The probl
Electronics Forum | Fri May 14 11:17:42 EDT 2004 | Ashok Dhawan
I am having coating adhesion problem with flex circuits. The cover plate material is KAPTON or Poly imide. The conformal coating material used is humiseal 2A64. The boards are cleaned, measuring less than 4 microgram Nacl per sq in. against acceptabl
Electronics Forum | Fri Sep 17 09:31:17 EDT 2004 | russ
Step stencils are used but only when necessary. One reason to use one would be a PCB with 12 mil pitch and very large coils or something of that nature. The 12 mil pitch part would require a 4 mil thick stencil to ensure release while it would caus