Electronics Forum | Tue Mar 04 18:38:12 EST 2003 | ruggi
Most of what we do (across 800+ varieties) is bottom side first. In general, there really aren't any problems as long as our Customers follow the .25g/cm wetted lead perimeter spec for weight (which many don't), and don't mount tall components on th
Electronics Forum | Wed Sep 17 08:41:28 EDT 2003 | caldon
In addition, I also think it would be detrimental in the double sided reflow process. Cal
Electronics Forum | Wed Sep 17 12:30:09 EDT 2003 | russ
I can guarantee that vibrating ovens will be detrimental in double sided reflow for any of the larger parts. I find it interesting about BTU and there "vibrating" oven. I had a couple of these in the early days and they did indeed vibrate. However
Electronics Forum | Thu Jul 05 11:26:08 EDT 2012 | cobham1
I need help with how long do I need to bake out double sided PCB's that have been cleaned. The units will not be reworked but instead will be moved on to hand stuffing. I have looked in IPC CH-65B and J-STD-033C. I get information for parts if I am r
Electronics Forum | Fri Feb 13 03:53:40 EST 1998 | Brian S. Bentzen
Hi , I have not been able to find any good description on how to perform double sided reflow on PCBs.The best would of course be to avoid reflowing the bottom side again but in real life this is not possible. So when double sided reflow soldering
Electronics Forum | Tue Oct 07 08:44:49 EDT 2014 | emeto
Hi, 1. I will run the board on the mesh if single sided. 2. For double sided board, I will try stiffeners. 3. If stiffeners don't work, then you have to create a handling fixture(holds the board and has enough openings to let the air flow to the PC
Electronics Forum | Wed Feb 18 12:08:04 EST 1998 | Eyal Epstein
Hi, I am from Celtronix Ltd. we are a provider of Odd Form assembly equipment and have gained a lot of experience in double side reflow, both the chemical side of it as well as the automatic insertion of all types of TH components in paste. Enclosed
Electronics Forum | Thu Oct 08 22:32:53 EDT 1998 | E.
*Reply to: ericr@nj.tanon.com Without going into a lengthy explaination {at this time}, has anyone experimented, tested, evaluate, and/or 'perfected' an SMT double-side reflow process. Presently I'm using a Kester R593 OA (water soluble) Sn63/Pb37 -
Electronics Forum | Mon Jun 18 10:11:52 EDT 2007 | dyoungquist
Almost every board/panel we build is double sided and we use an MPM SPM screen printer with no problems. The screen printer is not the cause. We have seen heavier parts fall off the first side when going through the reflow for the second side. We
Electronics Forum | Fri Feb 13 08:54:43 EST 1998 | justin medernach
| Hi , | I have not been able to find any good description on how to perform double sided reflow on PCBs.The best would of course be to avoid reflowing the bottom side again but in real life this is not possible. | So when double sided reflow sol