Electronics Forum | Sun Jan 31 03:28:24 EST 1999 | Jeff Sanchez
| Hello Netters, | | I need some info, Earl or Dave, I have a PCB that exhibits a white layer on solder side. It does not appear to be surface residues (IPA has no effect), but looks like its under solder mask. My first guess is that the LPI solde
Electronics Forum | Thu Apr 22 20:26:39 EDT 1999 | Dave F
| | On various PCB's after building processes,such as reflow, flowsolder and wash. The soldermask on the PCB's have become discoloured, like a 'marble' effect all along the solder side of the board, it is lighter in contrast than normal, although whe
Electronics Forum | Thu Jan 28 14:10:57 EST 1999 | Tom B
Hello Netters, I need some info, Earl or Dave, I have a PCB that exhibits a white layer on solder side. It does not appear to be surface residues (IPA has no effect), but looks like its under solder mask. My first guess is that the LPI solder mask
Electronics Forum | Thu Jan 28 15:43:16 EST 1999 | Dave F
| Hello Netters, | | I need some info, Earl or Dave, I have a PCB that exhibits a white layer on solder side. It does not appear to be surface residues (IPA has no effect), but looks like its under solder mask. My first guess is that the LPI solde
Electronics Forum | Sat May 29 16:56:26 EDT 1999 | Jeff Sanchez
| | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processing a double-
Electronics Forum | Sun May 30 10:15:34 EDT 1999 | Vic Lau
| | | | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processing a dou
Electronics Forum | Thu Jan 28 15:53:12 EST 1999 | Dave F
| | Hello Netters, | | | | I need some info, Earl or Dave, I have a PCB that exhibits a white layer on solder side. It does not appear to be surface residues (IPA has no effect), but looks like its under solder mask. My first guess is that the LPI
Electronics Forum | Sun May 30 18:52:35 EDT 1999 | Graham Naisbitt
| | | | | | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processing a
Electronics Forum | Thu Jan 28 16:29:03 EST 1999 | Tom B
Okay, Another question, if the soldermask in not cured, then it is washed will water ingress (from wash or ambient ) play havoc with capacitance or dielectric of PCB. I mean will my crystal and clock circuits start "Y2K'n" on me. OR will my PCB go
Electronics Forum | Thu Jan 28 17:31:20 EST 1999 | Earl Moon
| | | Hello Netters, | | | | | | I need some info, Earl or Dave, I have a PCB that exhibits a white layer on solder side. It does not appear to be surface residues (IPA has no effect), but looks like its under solder mask. My first guess is that t