Electronics Forum | Thu Jan 14 13:25:53 EST 1999 | Chrys
| Hi Folks. Has any Process Engineer here done a complete evaluation or controlled experiment for VOC-FREE Flux? Our goal here at CEBUKid, Inc. is to implement a VOC-FREE process. We have all the necessary (OPTIFLUX) spray equipment, and we're cur
Electronics Forum | Mon Feb 22 16:39:33 EST 1999 | C.K.
| | Hi Folks. Has any Process Engineer here done a complete evaluation or controlled experiment for VOC-FREE Flux? Our goal here at CEBUKid, Inc. is to implement a VOC-FREE process. We have all the necessary (OPTIFLUX) spray equipment, and we're c
Electronics Forum | Fri Dec 18 10:18:55 EST 1998 | Dave F
| I have been developing a BGA Process and are having problems with a 310 IO PBGA reflowing. I am achieving good wetting exept 2 to 5 balls on the outer perimeter I have a good profile my air flow is set per mfg spec, the strange thing is that it doe
Electronics Forum | Wed Dec 23 11:11:07 EST 1998 | john watt
| | I have been developing a BGA Process and are having problems with a 310 IO PBGA reflowing. I am achieving good wetting exept 2 to 5 balls on the outer perimeter I have a good profile my air flow is set per mfg spec, the strange thing is that it d
Electronics Forum | Tue Dec 01 14:44:04 EST 1998 | Terry Burnette
| Hi | I have been conducting my first reflow profiles. Most of the texts that I have read suggest soldering the thermocouples to a populated pcb. I am finding this very difficult. I have been using a high melting point (Sn5 / Pb95) solder and the
Electronics Forum | Tue Oct 06 17:17:44 EDT 1998 | Chrys
| We are experiencing poor wetting on various components placed on a PCB with En-Tek coating. Is anyone else experiencing simular problems ? We have the following questions: | | 1. How can the thickness of the En-tek coating be measured? | 2. Is En
Electronics Forum | Mon Sep 28 19:07:47 EDT 1998 | Steve Gregory
| I have had some field failures returned recently, the boards had flux contamination under the components in a sensitive area, Nothing really visible until the component was removed, and the board had no evidence of rework of any type. Is it poss
Electronics Forum | Tue Sep 22 12:25:31 EDT 1998 | Chrys
| | Hi Jacqueline! | | Do these joints that you're having problems with happen to be on fine pitch solder joints? Are the fillets staying attached to the foot and separating from the pads cleanly? | | If that is true, are there many vias concen
Electronics Forum | Fri Aug 21 07:57:20 EDT 1998 | Earl Moon
| | | Will somebody please explain HASL (here). Thanks. | | Tryin: HASL: Hot Air Solder Leveled. A board fabrication process that applies an oxidation preventing solder coating to copper pads on the board. Dave F | You do this to keep the green s
Electronics Forum | Fri Aug 14 07:27:42 EDT 1998 | Earl Moon
| | Hi, can you please tell me how to make green coating and through-hole plating of PCB? Thanks! | | Xingsheng | Xingsheng: Welcome. | Bible on PCB fabrication: Printed Circuits Handbook, Clyde Coombs, McGraw-Hill | Web resources: http://www.pw